公开(公告)号:US09245680B2
公开(公告)日:2016-01-26
申请号:US13601889
申请日:2012-08-31
申请人: Miho Kitamura , Hayami Kudo , Atsushi Yamamoto , Akihiro Nakamura
发明人: Miho Kitamura , Hayami Kudo , Atsushi Yamamoto , Akihiro Nakamura
CPC分类号: H01F17/0013 , H01F41/04 , H01F41/046 , H01F2017/008 , Y10T29/49075
摘要: There is provided a common mode choke coil in which a non-magnetic layer and a second magnetic layer stacked on a first magnetic layer and two facing conductive coils are included in the non-magnetic layer, the non-magnetic layer is formed of sintered glass ceramics, the conductive coils and are formed of a conductor containing copper, and at least one of the first magnetic layer and the second magnetic layer is formed of a sintered ferrite material containing Fe2O3, Mn2O3, NiO, ZnO and CuO. The sintered ferrite material has an Fe2O3-reduced content of 25 to 47 mol % and a Mn2O3-reduced content of 1 to 7.5 mol %, or Fe2O3-reduced content of 35 to 45 mol % and a Mn2O3-reduced content of 7.5 to 10 mol %, and a CuO reduced content of 5 mol %.
摘要翻译: 提供了一种共模扼流线圈,其中堆叠在第一磁性层上的非磁性层和第二磁性层和两个面对的导电线圈包括在非磁性层中,非磁性层由烧结玻璃形成 陶瓷,导电线圈,由含有铜的导体形成,并且第一磁性层和第二磁性层中的至少一个由含有Fe 2 O 3,Mn 2 O 3,NiO,ZnO和CuO的烧结铁氧体材料形成。 烧结铁氧体材料的Fe 2 O 3还原含量为25〜47摩尔%,Mn2O3还原含量为1〜7.5摩尔%,Fe2O3还原含量为35〜45摩尔%,Mn2O3还原含量为7.5〜10 mol%,CuO还原含量为5mol%。