Oil-impregnated sintered bearing
    1.
    发明申请
    Oil-impregnated sintered bearing 审中-公开
    浸油烧结轴承

    公开(公告)号:US20060269179A1

    公开(公告)日:2006-11-30

    申请号:US10561221

    申请日:2004-06-09

    IPC分类号: F16C33/02

    CPC分类号: F16C23/045 F16C33/103

    摘要: An object of the present invention is to provide an oil-impregnated sintered sliding bearing which has a large amount of the lubricating oil as a bearing element which has long life, has a small amount of scattered and lost lubricating oil, has a simple structure, and takes up a small space for a bearing. An oil-impregnated sintered sliding bearing includes: an axis; plural porous sintered compacts joined with each other by sizing; a cavity between the sintered compacts at an axial direction center portion; and a gap which continuously extends from an end portion of the cavity and has a width narrower than the cavity, wherein the gap opens to an end surface or a peripheral surface of the bearing.

    摘要翻译: 本发明的目的是提供一种油浸烧结滑动轴承,其具有大量的润滑油作为轴承元件,其使用寿命长,具有少量的散失和损失的润滑油,结构简单, 并占据了一个很小的轴承空间。 油浸式烧结滑动轴承包括:轴; 多个多孔烧结体通过施胶相互结合; 在轴向中心部分的烧结体之间的空腔; 以及从空腔的端部连续延伸并且具有比空腔窄的宽度的间隙,其中间隙通向轴承的端面或外周表面。

    METHOD OF MANUFACTURING BLADE RUBBER AND WIPER BLADE
    2.
    发明申请
    METHOD OF MANUFACTURING BLADE RUBBER AND WIPER BLADE 有权
    制造叶片橡胶和刮刀叶片的方法

    公开(公告)号:US20110119857A1

    公开(公告)日:2011-05-26

    申请号:US13055057

    申请日:2009-07-17

    IPC分类号: B60S1/38 B29C47/00

    摘要: A blade rubber having both of superior durability and wiping performance can be manufactured by using a non-diene-based rubber without environmental burden. A pair of blade-rubber molded bodies molded from the non-diene-based rubber is subjected to an irradiation treatment to generate radical active sites, and monomers are bound by graft polymerization as beginning at the radical active sites. Also, the monomers are adhered on a surface of the blade rubber either before or after the generation of the radical active sites. The irradiation treatment and the graft polymerization may be simultaneously performed or independently performed in this order. In this manner, a surface treatment for reducing friction of the non-diene-based rubber having superior durability can be performed without halogen, and therefore, a blade rubber having superior durability and wiping performance can be manufactured.

    摘要翻译: 具有优异的耐久性和擦拭性能的刀片橡胶可以通过使用不带环境负荷的非二烯类橡胶来制造。 对由非二烯类橡胶成型的一对刀片橡胶成型体进行照射处理,生成自由基活性部位,单体在自由基活性部位开始接枝聚合。 此外,单体在产生基团活性部位之前或之后粘附在刮片橡胶的表面上。 照射处理和接枝聚合可以按顺序同时进行或独立地进行。 以这种方式,可以在没有卤素的情况下进行用于降低耐久性优异的非二烯系橡胶的摩擦的表面处理,因此,可以制造具有优异的耐久性和擦拭性能的刮板橡胶。

    Surface-modified blade rubber, wiper unit, and blade rubber surface modifying method
    3.
    发明申请
    Surface-modified blade rubber, wiper unit, and blade rubber surface modifying method 有权
    表面改性叶片橡胶,刮水器单元和叶片橡胶表面改性方法

    公开(公告)号:US20080016644A1

    公开(公告)日:2008-01-24

    申请号:US11826288

    申请日:2007-07-13

    IPC分类号: B60S1/38 C08F2/46

    摘要: A surface-modified blade rubber includes a surface modified by being subjected to irradiation treatment that generates radical active sites in the blade rubber and polymerization for graft polymerization starting from a generated radical active site. A method for modifying a blade rubber surface includes subjecting rubber of a blade rubber to irradiation treatment that generates radical active sites and polymerization for graft polymerization starting from a generated radical active site.

    摘要翻译: 表面改性的刮板橡胶包括通过经受辐照处理而改性的表面,其在所述刮片橡胶中产生自由基活性位点,并且从所产生的活性位点开始接枝聚合的聚合。 用于改变叶片橡胶表面的方法包括:从所产生的活性部位开始,对刮片橡胶的橡胶进行产生自由基活性部位的辐射处理和接枝聚合的聚合。

    Method of manufacturing blade rubber and wiper blade
    4.
    发明授权
    Method of manufacturing blade rubber and wiper blade 有权
    制造叶片橡胶和刮水片的方法

    公开(公告)号:US08679638B2

    公开(公告)日:2014-03-25

    申请号:US13055057

    申请日:2009-07-17

    IPC分类号: B32B27/00

    摘要: A blade rubber having both of superior durability and wiping performance can be manufactured by using a non-diene-based rubber without environmental burden. A pair of blade-rubber molded bodies molded from the non-diene-based rubber is subjected to an irradiation treatment to generate radical active sites, and monomers are bound by graft polymerization as beginning at the radical active sites. Also, the monomers are adhered on a surface of the blade rubber either before or after the generation of the radical active sites. The irradiation treatment and the graft polymerization may be simultaneously performed or independently performed in this order. In this manner, a surface treatment for reducing friction of the non-diene-based rubber having superior durability can be performed without halogen, and therefore, a blade rubber having superior durability and wiping performance can be manufactured.

    摘要翻译: 具有优异的耐久性和擦拭性能的刀片橡胶可以通过使用不带环境负荷的非二烯类橡胶来制造。 对由非二烯类橡胶成型的一对刀片橡胶成型体进行照射处理,生成自由基活性部位,单体在自由基活性部位开始接枝聚合。 此外,单体在产生基团活性部位之前或之后粘附在刮片橡胶的表面上。 照射处理和接枝聚合可以按顺序同时进行或独立地进行。 以这种方式,可以在没有卤素的情况下进行用于降低耐久性优异的非二烯系橡胶的摩擦的表面处理,因此,可以制造具有优异的耐久性和擦拭性能的刮板橡胶。

    Surface-modified blade rubber, wiper unit, and blade rubber surface modifying method
    6.
    发明授权
    Surface-modified blade rubber, wiper unit, and blade rubber surface modifying method 有权
    表面改性叶片橡胶,刮水器单元和叶片橡胶表面改性方法

    公开(公告)号:US08227522B2

    公开(公告)日:2012-07-24

    申请号:US11826288

    申请日:2007-07-13

    摘要: A surface-modified blade rubber includes a surface modified by being subjected to irradiation treatment that generates radical active sites in the blade rubber and polymerization for graft polymerization starting from a generated radical active site. A method for modifying a blade rubber surface includes subjecting rubber of a blade rubber to irradiation treatment that generates radical active sites and polymerization for graft polymerization starting from a generated radical active site.

    摘要翻译: 表面改性的刮板橡胶包括通过经受辐照处理而改性的表面,其在所述刮片橡胶中产生自由基活性位点,并且从所产生的活性位点开始接枝聚合的聚合。 用于改变叶片橡胶表面的方法包括:从所产生的活性部位开始,对刮片橡胶的橡胶进行产生自由基活性部位的辐射处理和接枝聚合的聚合。