公开(公告)号:US10822277B2
公开(公告)日:2020-11-03
申请号:US15736456
申请日:2016-06-13
Applicant: National Institute for Materials Science
Inventor: Toshio Osada , Kiichi Kamoda , Toru Hara , Masanori Mitome , Taichi Abe , Takahito Ohmura , Wataru Nakao
IPC: C04B35/117 , C04B35/78 , C04B35/185 , C04B35/10 , C04B35/63 , C04B35/645 , F01D5/28 , F01D9/04 , F01D25/00 , C04B35/577
Abstract: The present invention relates to an oxidation-induced highly-functional self-healing ceramic composition, a method for producing the ceramic composition, a use of the ceramic composition and a method for achieving the enhancement of the functionality of the ceramic composition, by focusing on a repairing stage and a remodeling state in a self-healing process and by carrying out elemental and structural designing of an oxidation-induced self-healing ceramic composition for the purpose of speeding up these stages.
-
公开(公告)号:US09945019B2
公开(公告)日:2018-04-17
申请号:US15372500
申请日:2016-12-08
Applicant: NATIONAL INSTITUTE FOR MATERIALS SCIENCE
Inventor: Yuefeng Gu , Toshio Osada , Yong Yuan , Tadaharu Yokokawa , Hiroshi Harada
CPC classification number: C22F1/10 , B21J5/02 , C22C19/05 , C22C19/056 , C22C19/07 , C22C30/00 , C22F1/00 , F01D5/02 , F01D5/28 , F05D2300/175
Abstract: Disclosed herein is a nickel-based heat-resistant superalloy produced by a casting and forging method, the nickel-based heat-resistant superalloy comprising 2.0 mass % or more but 25 mass % or less of chromium, 0.2 mass % or more but 7.0 mass % or less of aluminum, 19.5 mass % or more but 55.0 mass % or less of cobalt, [0.17×(mass % of cobalt content−23)+3] mass % or more but [0.17×(mass % of cobalt content−20)+7] mass % or less and 5.1 mass % or more of titanium, and the balance being nickel and inevitable impurities, and being subjected to solution heat treatment at 93% or more but less than 100% of a γ′ solvus temperature.
-