Process for producing metal flakes
    3.
    发明授权
    Process for producing metal flakes 失效
    生产金属薄片的方法

    公开(公告)号:US4743297A

    公开(公告)日:1988-05-10

    申请号:US33708

    申请日:1987-04-03

    IPC分类号: B22F1/00 B22F9/04

    摘要: A process is disclosed for producing metal flakes. The process involves entraining the metal powder particles in a carrier gas and passing the powder particles through a high temperature zone at a temperature above the melting point of the powder particles to melt at least about 50% of the powder particles, resolidifying the resulting high temperature treated material by impacting the material against a substrate, and thereafter contacting the material with a non-oxidizing gas which can be nitrogen, argon, hydrogen, helium or combinations of these to remove the material from the substrate in the form of flakes.

    摘要翻译: 公开了一种用于生产金属薄片的方法。 该方法包括将金属粉末颗粒夹带在载气中,并使粉末颗粒在高于粉末颗粒熔点的温度下通过高温区域,以熔化至少约50%的粉末颗粒,将所得到的高温 然后将材料与非氧化性气体接触,所述非氧化性气体可以是氮气,氩气,氢气,氦气或这些材料的组合,以从薄片形式从衬底去除材料。

    Process for producing finely divided spherical metal powders
    4.
    发明授权
    Process for producing finely divided spherical metal powders 失效
    用于生产精细分散的球形金属粉末的方法

    公开(公告)号:US4670047A

    公开(公告)日:1987-06-02

    申请号:US906370

    申请日:1986-09-12

    IPC分类号: B22F1/00 B22F9/00

    CPC分类号: B22F1/0048 B22F2998/10

    摘要: A process is disclosed for producing finely divided spherical metal powders. The process comprises forming a coating of a surface active agent which can be of the nonionic or anionic type on the surfaces of the particles of a metal powder, feeding the coated particles and a carrier gas into a high temperature zone and maintaining the particles in the zone for a sufficient time to melt at least about 50% by weight of the particles and to form droplets therefrom, and cooling the droplets to form metal particles having essentially a spherical shape with the majority of the particles having a size less than about 50 micrometers.

    摘要翻译: 公开了一种用于生产精细分散的球形金属粉末的方法。 该方法包括在金属粉末颗粒的表面上形成可以是非离子或阴离子型表面活性剂的涂层,将涂覆的颗粒和载气进料到高温区并将颗粒保持在 区域足以熔化至少约50重量%的颗粒并从其形成液滴,并冷却液滴以形成具有基本上为球形的金属颗粒,其中大部分颗粒的尺寸小于约50微米 。