摘要:
A glass panel for a cathode ray tube comprises a substantially rectangular face portion on which images are displayed and a skirt portion continuous to the face portion through a blend R portion. An effective screen size of the face portion in a diagonal direction is 500 mm or more, an average radius of curvature of an outer surface of the face portion is 10000 mm or more in all radial directions from a face center portion, and a difference in height between the face center portion and an edge portion of the effective screen in the diagonal direction on an inner surface of the face portion is in a range from 9 mm to 17 mm.
摘要:
A cathode-ray tube panel, wherein the outer surface (12) of the cathode-ray tube panel (10) is made in the form of a roughened surface (14) having microscopic irregularities and the roughened surface is formed with a thin electrically conductive film (15) made of SnO.sub.2 and Sb.sub.2 O.sub.3, thereby making the panel both antistatic and antireflective.
摘要:
A panel glass of a color cathode ray tube exhibiting a high absorption of X-radiation and an excellent resistance to electron and/or X-ray browning, which is modified by 0.1-5.0 wt % Nd.sub.2 0.sub.3 to provide substantially higher relative light transmission in the green and in the red wavelengths of the visible spectrum and a greater selective light absorption in the yellow region of the spectrum, and which is further modified by 0.0005-0.05 wt % Cr.sub.2 O.sub.3 and 0-2 wt % Pr.sub.6 O.sub.11 to control the chromaticity value of the glass to be nearly equal to that of the light emitted from tricolor phosphor P22 and to suppress the dichroism of the glass for different ambient lights. Ingredients of the glass are as follows: 50-75% SiO.sub.2, 0-5% Al.sub.2 O.sub.3, 0-4% CaO, 0-3% MgO, 0-13% SrO, 0-16% BaO, 0-3% PbO, O-3% ZnO, 0-4% ZrO.sub.2, the sum of SrO+BaO+PbO+ZnO+ZrO.sub.2 being 5-25%, 0-4% Li.sub.2 O, 3-15% Na.sub.2 O, 2-15% K.sub.2 O, the sum of Na.sub.2 O+K.sub.2 O being 5-20%, O-2%, TiO.sub.2, O-3% CeO.sub.2, 0.1-5.0% Nd.sub.2 O.sub.3, 0.0005-0.05% Cr.sub.2 O.sub.3, and 0-2% Pr.sub.6 O.sub.11.
摘要翻译:显示出高吸收X射线和优异的抗电子和/或X射线褐变的彩色阴极射线管的面板玻璃,其被0.1-5.0重量%的Nd 2 O 3改性,以提供更高的相对光透射率 绿色和可见光谱的红色波长,并且在光谱的黄色区域具有更大的选择性光吸收,并进一步改性为0.0005-0.05重量%的Cr2O3和0-2重量%的Pr6O11,以控制色度值 玻璃几乎等于从三色荧光体P22发出的光的玻璃,并抑制不同环境光的玻璃的二色性。 玻璃的成分如下:50-75%SiO 2,0-5%Al 2 O 3,0-4%CaO,0-3%MgO,0-13%SrO,0-16%BaO,0-3%PbO, O-3%ZnO,0-4%ZrO2,SrO + BaO + PbO + ZnO + ZrO2的总和为5-25%,0-4%Li2O,3-15%Na2O,2-15%K2O,总和 的Na2O + K2O为5-20%,O-2%,TiO2,O-3%CeO2,0.1-5.0%Nd2O3,0.0005-0.05%Cr2O3和0-2%Pr6O11。
摘要:
In a plurality of monochromatic colored light emitted cathode ray tubes arranged in a surface to form a huge screen for displaying a colored picture, glass for use in light-source cathode ray tubes for emitting the red or the blue light has the optical characteristics that it can well pass the light in the wavelength range of the remaining blue and yellow portions of the spectrum to thereby improve contrast of the monochromatic colored red or green light source cathode ray tube. The glass essentially consists, by weight, of 50-75% SiO.sub.2, O-5% Al.sub.2 O.sub.3, 0-4% CaO, 0-2% MgO, 0-12% SrO, 0-16% BaO, 0-3% PbO, 0-3% ZnO, 0-3% ZrO.sub.2, the sum of SrO+BaO+PbO+ZnO+ZrO.sub.2 being 1.5-25%, 0-4% Li.sub.2 O, 3-15% Na.sub.2 O, 1-10% K.sub.2 O, the sum of Li.sub.2 O+Na.sub.2 O+K.sub.2 O being 5-24%, 0-2% TiO.sub.2, 0.1-3% CeO.sub.2, 1-10% Nd.sub.2 O.sub.3, 0.5-5% Pr.sub.2 O.sub.3, and 0.1-4% Fe.sub.2 O.sub.3. According to the glass, the red light emitting cathode ray tube and the green light emitting cathode ray tube are produced only by a simple kind of glass without sacrificing contrast characteristic of the light-source cathode ray tubes emitting red light and green light, respectively. Thus, the red light emitting and the green light emitting cathode ray tubes using the glass are used together with the blue light emitting cathode ray tube to form a huge screen with a reduced cost and without pollution.