摘要:
This invention relates to the use of olefin mixtures containing 1-hexene/1-decene/1-dodecene and, additionally, 1-octene or 1-decene to produce high viscosity polyalphaolefins (PAOs) having a viscosity of from about 40 cSt to about 100 cSt at 100° C. (ASTM D-445) and a number average molecular weight of between about 1200 to about 4000, particularly useful as lubricant base stocks.
摘要:
The invention relates to a method of making a PAO characterized by a low viscosity, low Noack volatility, and excellent cold temperature properties, using a promoter system comprising an alcohol and an ester. The products comprise trimers obtained by fractionating a hydrogenated bottoms product from an oligomerization process using said promoter system.
摘要:
The invention relates to a method of making a PAO from mixtures comprising 1-decene and 1-dodecene, characterized by a low viscosity and excellent cold temperature properties, using a promoter system comprising an alcohol. In embodiments, the product has properties similar to those obtainable using a feed of solely 1-decene.
摘要:
Disclosed herein is a method of making a PAO using tetradecene and particularly mixtures comprising 1-hexene, 1-decene, 1-dodecene, and 1-tetradecene, characterized by a low viscosity and excellent cold temperature properties, using a promoter system comprising an alcohol and an ester. In embodiments, the product has properties similar to those obtainable using a feed of solely 1-decene.
摘要:
This invention relates to the use of 1-decene/1-dodecene olefin mixture to produce high viscosity polyalphaolefins (PAOs) having a viscosity of from about 40 cSt to about 100 cSt at 100° C. (ASTM D-445) and a number average molecular weight of between about 1200 to about 4000, particularly useful as lubricant base stocks.