METHOD FOR MANUFACTURING GRAIN-ORIENTED ELECTRICAL STEEL SHEET

    公开(公告)号:US20190017140A1

    公开(公告)日:2019-01-17

    申请号:US16065002

    申请日:2016-12-20

    申请人: POSCO

    摘要: A manufacturing method of an oriented electrical steel sheet according to an exemplary embodiment of the present invention includes: a step of manufacturing a steel slab including one kind or more among Si at 2 to 7%, Sn at 0.03 to 0.10%, and Sb at 0.01 to 0.05% as wt %; a step of hot-rolling the steel slab to manufacture a hot rolled sheet; a step of cold-rolling the hot rolled sheet to manufacture a cold rolled sheet; a step of decarburizing and nitriding the cold rolled sheet for primary recrystallization annealing; a step of coating and drying an annealing separating agent on the primary recrystallization-annealed cold rolled sheet; and a step of secondary recrystallization-annealing the cold rolled sheet coated with the annealing separating agent.

    METHOD FOR MANUFACTURING GRAIN-ORIENTED ELECTRICAL STEEL SHEET

    公开(公告)号:US20190010572A1

    公开(公告)日:2019-01-10

    申请号:US16065774

    申请日:2016-12-23

    申请人: POSCO

    摘要: A method for manufacturing grain-oriented electrical steel sheet comprises: manufacturing a steel slab comprising at least one of 2 wt % to 7 wt % of Si, 0.03 wt % to 0.10 wt % of Sn, and 0.01 wt % to 0.05 wt % of Sb; hot-rolling the steel slab to produce a hot-rolled sheet; cold-rolling the hot-rolled sheet to produce a cold-rolled sheet; primary recrystallization-annealing the cold-rolled sheet; applying an annealing separator to the primary recrystallization-annealed cold-rolled sheet and drying the same; and secondary recrystallization-annealing the cold-rolled sheet on which the annealing separator is applied. The primary recrystallization-annealing is performed so that the thickness of an oxide layer formed on the surface of the cold-rolled sheet is 0.5 μm to 2.5 μm, and the oxygen amount of the oxide layer is 600 ppm or more after the primary recrystallization-annealing, and in which a forsterite (Mg2SiO4) film can be removed in the secondary recrystallization-annealing.

    ORIENTED ELECTRICAL STEEL SHEET AND METHOD FOR PREPARING SAME

    公开(公告)号:US20210062309A1

    公开(公告)日:2021-03-04

    申请号:US16957943

    申请日:2018-05-17

    申请人: POSCO

    摘要: An oriented electrical steel sheet according to an embodiment of the present invention includes, in a unit of wt %, Si at 1.0 wt % to 5.0 wt %, C at 0.005 wt % or less (excluding 0 wt %), Mn at 0.001 wt % to 0.1 wt %, Cu at 0.001 wt % to 0.1 wt %, S at 0.001 wt % to 0.020 wt %, Se at 0.001 wt % to 0.050 wt %, Al at 0.0005 wt % to 0.010 wt %, N at 0.0005 wt % to 0.005 wt %, and the remainder of Fe and inevitable impurities.
    The oriented electrical steel sheet according to the embodiment of the present invention satisfies Equation 1. 16≤(10×[Mn]+[Cu])/([S]+[Se])+(0.02−[Al])/[N]≤20   [Equation 1] (In Equation 1, [Mn], [Cu], [S], [Se], [Al], and [N] represent contents (wt %) of Mn, Cu, S, Se, Al, and N, respectively.)