ALL-SOLID BATTERY
    1.
    发明申请
    ALL-SOLID BATTERY 审中-公开

    公开(公告)号:US20200212499A1

    公开(公告)日:2020-07-02

    申请号:US16714604

    申请日:2019-12-13

    Abstract: An all-solid battery includes a positive-electrode layer having a positive-electrode current collector and a positive-electrode mixture layer, a negative-electrode layer having a negative-electrode current collector and a negative-electrode mixture layer, and a solid electrolyte layer. The positive-electrode mixture layer contains a positive-electrode active material and a solid electrolyte. The solid electrolyte layer is disposed between the positive-electrode mixture layer and the negative-electrode mixture layer. In the positive-electrode mixture layer, the active material volume proportion is larger and the porosity is smaller in a portion closer to the positive-electrode current collector than in a portion far from the positive-electrode current collector.

    ALL-SOLID BATTERY AND METHOD OF MANUFACTURING THE SAME

    公开(公告)号:US20200212479A1

    公开(公告)日:2020-07-02

    申请号:US16714593

    申请日:2019-12-13

    Abstract: An all-solid battery includes a positive-electrode layer, a negative-electrode layer, and a solid electrolyte layer. The positive-electrode layer includes a positive-electrode current collector, a positive-electrode bonding layer that contains at least a conductive agent comprising non-metal and is formed on the positive-electrode current collector, and a positive-electrode mixture layer that contains at least a positive-electrode active material and a solid electrolyte and is formed on the positive-electrode bonding layer. The negative-electrode layer includes a negative-electrode current collector and a negative-electrode mixture layer that contains at least a negative-electrode active material and the solid electrolyte. The solid electrolyte layer is disposed between the positive-electrode mixture layer and the negative-electrode mixture layer and contains the solid electrolyte. A concentration of a binder contained in the positive-electrode mixture layer is less than or equal to 100 ppm and a concentration of a solvent contained in the positive-electrode mixture layer is less than or equal to 50 ppm.

Patent Agency Ranking