1.
公开(公告)号:US20090226636A1
公开(公告)日:2009-09-10
申请号:US12399648
申请日:2009-03-06
申请人: Patrick LEBLANC , Frederic COTTON , Dave LESSARD , Alain VALLEE
发明人: Patrick LEBLANC , Frederic COTTON , Dave LESSARD , Alain VALLEE
CPC分类号: H01M4/139 , H01M4/0404
摘要: A process for making an electrode sheet for lithium electrochemical cells is disclosed. The process comprises the steps of: a) admixing a polyether polymer or copolymer soluble in water, at least one lithium salt, at least one electrochemically active material, water and an organic solvent miscible with water in a water/organic solvent ratio of a maximum of 50% organic solvent by volume to form a water-based solution/suspension containing by weight at least 20% active electrode material, at least 5% of a polyether polymer or copolymer, and at least 1.5% lithium salt; b) coating the water-based solution/suspension in the form of an electrode thin film onto an electrode support; and, c) drying the electrode thin film to obtain an electrode thin sheet having less than 1000 ppm of residual water.
摘要翻译: 公开了一种制造锂电池的电极片的方法。 该方法包括以下步骤:a)将可溶于水的聚醚聚合物或共聚物,至少一种锂盐,至少一种电化学活性材料,水和与水混合的有机溶剂与水/有机溶剂的最大比例混合, 的50%有机溶剂,以形成含有至少20%活性电极材料,至少5%的聚醚聚合物或共聚物和至少1.5%的锂盐的水基溶液/悬浮液; b)将电极薄膜形式的水性溶液/悬浮液涂布到电极载体上; c)干燥电极薄膜,得到残留水小于1000ppm的电极薄片。
-
2.
公开(公告)号:US20090226635A1
公开(公告)日:2009-09-10
申请号:US12044612
申请日:2008-03-07
申请人: Patrick LEBLANC , Frederic COTTON , Dave LESSARD , Alain VALLEE
发明人: Patrick LEBLANC , Frederic COTTON , Dave LESSARD , Alain VALLEE
CPC分类号: H01M4/0404 , H01M4/0416 , H01M4/139 , H01M4/485 , H01M4/505 , H01M4/525 , H01M4/622
摘要: A process for making an electrode sheet for a solid lithium electrochemical cells is disclosed. The process comprises the steps of: a) admixing a polyether polymer or copolymer, at least one lithium salt, at least one electrochemically active material and purified water to form an aqueous solution/suspension containing by weight at least 40% purified water, at least 20% active electrode material, up to 10% electrically conductive material, at least 5% polyether polymer or copolymer, and at least 1.5% lithium salt; b) coating the aqueous solution/suspension in the form of an electrode thin film onto an electrode support; and, c) evaporating the water from the electrode thin film to obtain an electrode sheet having less than 1000 ppm of residual water. The evaporation step is preferably carried out through a dryer/oven tunnel having incremental drying zones.
摘要翻译: 公开了制备固体锂电池的电极片的方法。 该方法包括以下步骤:a)将聚醚聚合物或共聚物,至少一种锂盐,至少一种电化学活性材料和纯化水混合,形成至少含有至少40%净化水的水溶液/悬浮液,至少 20%的活性电极材料,高达10%的导电材料,至少5%的聚醚聚合物或共聚物,和至少1.5%的锂盐; b)将电极薄膜形式的水溶液/悬浮液涂覆到电极载体上; 并且c)从电极薄膜蒸发水以获得具有小于1000ppm残留水的电极片。 蒸发步骤优选通过具有增量干燥区的干燥器/烘箱通道进行。
-