1.
公开(公告)号:US11078325B2
公开(公告)日:2021-08-03
申请号:US16105161
申请日:2018-08-20
申请人: Presidium USA, Inc
发明人: James Henry Blumsom , Andrew John Tennant , James A. Cella , David Goldwasser , Daniel J. Brunelle , Stephen Burks , Richard Heggs
IPC分类号: C08G59/62 , C08G18/40 , C08G18/48 , C08G18/46 , C08G18/50 , C08G18/44 , C08G18/42 , C08G18/76 , C08G64/42 , C08G18/32 , C08G18/02 , C08L75/04
摘要: There is provided an oligomeric polyol composition having (a) an oligomeric network containing residues of at least one polyhydroxylated aromatic compound and residues of at least one polyol having at least three hydroxyl groups; and (b) a plurality of peripheral groups having one or more pendant hydroxyl groups bound to the oligomeric network by a plurality of linking units. The residues of the polyol may optionally contain one or more oxygen ether groups, one or more amino ether groups, or both of one or more oxygen ether groups and one or more amino ether groups. Reaction of the oligomeric polyols with isocyanate monomers affords a new class of polyurethanes having superior heat and water resistance. The new polyurethanes exhibit lower peak exotherms, typically less than 250° F. during in-mold polymerization. Articles prepared from polyurethanes incorporating such oligomeric polyol compositions exhibit flexural strengths and moduli in excess of 10,000 psi and 400,000 psi respectively, and outstanding green strength.
-
2.
公开(公告)号:US20190241699A1
公开(公告)日:2019-08-08
申请号:US16105161
申请日:2018-08-20
申请人: Presidium USA, Inc
发明人: James Henry Blumsom , Andrew John Tennant , James A. Cella , David Goldwasser , Daniel J. Brunelle , Stephen Burks , Richard Heggs
IPC分类号: C08G59/62 , C08G18/02 , C08G18/40 , C08G18/32 , C08G64/42 , C08G18/76 , C08L75/04 , C08G18/48 , C08G18/50 , C08G18/42 , C08G18/46 , C08G18/44
CPC分类号: C08G59/62 , C08G18/02 , C08G18/3206 , C08G18/3215 , C08G18/3284 , C08G18/40 , C08G18/4222 , C08G18/4244 , C08G18/44 , C08G18/46 , C08G18/4615 , C08G18/48 , C08G18/4829 , C08G18/5021 , C08G18/7664 , C08G64/42 , C08G2310/00 , C08J2375/04 , C08L75/04
摘要: There is provided an oligomeric polyol composition having (a) an oligomeric network containing residues of at least one polyhydroxylated aromatic compound and residues of at least one polyol having at least three hydroxyl groups; and (b) a plurality of peripheral groups having one or more pendant hydroxyl groups bound to the oligomeric network by a plurality of linking units. The residues of the polyol may optionally contain one or more oxygen ether groups, one or more amino ether groups, or both of one or more oxygen ether groups and one or more amino ether groups. Reaction of the oligomeric polyols with isocyanate monomers affords a new class of polyurethanes having superior heat and water resistance. The new polyurethanes exhibit lower peak exotherms, typically less than 250° F. during in-mold polymerization. Articles prepared from polyurethanes incorporating such oligomeric polyol compositions exhibit flexural strengths and moduli in excess of 10,000 psi and 400,000 psi respectively, and outstanding green strength.
-
公开(公告)号:US20190055345A1
公开(公告)日:2019-02-21
申请号:US16105106
申请日:2018-08-20
申请人: Presidium USA, Inc
发明人: James Henry Blumsom , Andrew John Tennant , James A. Cella , David Goldwasser , Daniel J. Brunelle , Stephen Burks , Richard Heggs
IPC分类号: C08G59/62 , C08G18/44 , C08G18/02 , C08G18/32 , C08G64/42 , C08G18/76 , C08G18/50 , C08G18/42 , C08G18/46 , C08G18/40 , C08G18/48 , C08L75/04
摘要: There is provided an oligomeric polyol composition having (a) an oligomeric network containing residues of at least one polyhydroxylated aromatic compound and residues of at least one polyol having at least three hydroxyl groups; and (b) a plurality of peripheral groups having one or more pendant hydroxyl groups bound to the oligomeric network by a plurality of linking units. The residues of the polyol may optionally contain one or more oxygen ether groups, one or more amino ether groups, or both of one or more oxygen ether groups and one or more amino ether groups. Reaction of the oligomeric polyols with isocyanate monomers affords a new class of polyurethanes having superior heat and water resistance. The new polyurethanes exhibit lower peak exotherms, typically less than 250° F. during in-mold polymerization. Articles prepared from polyurethanes incorporating such oligomeric polyol compositions exhibit flexural strengths and moduli in excess of 10,000 psi and 400,000 psi respectively, and outstanding green strength.
-
公开(公告)号:US10053533B1
公开(公告)日:2018-08-21
申请号:US15589182
申请日:2017-05-08
申请人: Presidium USA, Inc.
发明人: James Henry Blumsom , Andrew John Tennant , James A. Cella , David Goldwasser , Daniel J. Brunelle , Stephen Burks , Richard Heggs
IPC分类号: C08G59/62 , C08G18/42 , C08G18/40 , C08G18/46 , C08G18/48 , C08G18/50 , C08G18/44 , C08L75/04 , C08G18/02
CPC分类号: C08G59/62 , C08G18/02 , C08G18/3206 , C08G18/3215 , C08G18/3284 , C08G18/40 , C08G18/4222 , C08G18/4244 , C08G18/44 , C08G18/46 , C08G18/4615 , C08G18/48 , C08G18/4829 , C08G18/5021 , C08G18/7664 , C08G64/42 , C08G2310/00 , C08J2375/04 , C08L75/04
摘要: There is provided an oligomeric polyol composition having (a) an oligomeric network containing residues of at least one polyhydroxylated aromatic compound and residues of at least one polyol having at least three hydroxyl groups; and (b) a plurality of peripheral groups having one or more pendant hydroxyl groups bound to the oligomeric network by a plurality of linking units. The residues of the polyol may optionally contain one or more oxygen ether groups, one or more amino ether groups, or both one or more oxygen ether groups and one or more amino ether groups. Reaction of the oligomeric polyols with isocyanate monomers affords a new class of polyurethanes having superior heat and water resistance. The new polyurethanes exhibit lower peak exotherms, typically less than 250° F. during in-mold polymerization. Articles prepared from polyurethanes incorporating such oligomeric polyol compositions exhibit flexural strengths and moduli in excess of 10,000 psi and 400,000 psi respectively, and outstanding green strength.
-
公开(公告)号:US11072680B2
公开(公告)日:2021-07-27
申请号:US16105126
申请日:2018-08-20
申请人: Presidium USA, Inc
发明人: James Henry Blumsom , Andrew John Tennant , James A. Cella , David Goldwasser , Daniel J. Brunelle , Stephen Burks , Richard Heggs
IPC分类号: C08G59/62 , C08G18/40 , C08G18/48 , C08G18/46 , C08G18/50 , C08G18/44 , C08G18/42 , C08G18/76 , C08G64/42 , C08G18/32 , C08G18/02 , C08L75/04
摘要: There is provided an oligomeric polyol composition having (a) an oligomeric network containing residues of at least one polyhydroxylated aromatic compound and residues of at least one polyol having at least three hydroxyl groups; and (b) a plurality of peripheral groups having one or more pendant hydroxyl groups bound to the oligomeric network by a plurality of linking units. The residues of the polyol may optionally contain one or more oxygen ether groups, one or more amino ether groups, or both of one or more oxygen ether groups and one or more amino ether groups. Reaction of the oligomeric polyols with isocyanate monomers affords a new class of polyurethanes having superior heat and water resistance. The new polyurethanes exhibit lower peak exotherms, typically less than 250° F. during in-mold polymerization. Articles prepared from polyurethanes incorporating such oligomeric polyol compositions exhibit flexural strengths and moduli in excess of 10,000 psi and 400,000 psi respectively, and outstanding green strength.
-
公开(公告)号:US11066512B2
公开(公告)日:2021-07-20
申请号:US16105148
申请日:2018-08-20
申请人: Presidium USA, Inc
发明人: James Henry Blumsom , Andrew John Tennant , James A. Cella , David Goldwasser , Daniel J. Brunelle , Stephen Burks , Richard Heggs
IPC分类号: C08G59/62 , C08G18/40 , C08G18/48 , C08G18/46 , C08G18/50 , C08G18/44 , C08G18/42 , C08G18/76 , C08G64/42 , C08G18/32 , C08G18/02 , C08L75/04
摘要: There is provided an oligomeric polyol composition having (a) an oligomeric network containing residues of at least one polyhydroxylated aromatic compound and residues of at least one polyol having at least three hydroxyl groups; and (b) a plurality of peripheral groups having one or more pendant hydroxyl groups bound to the oligomeric network by a plurality of linking units. The residues of the polyol may optionally contain one or more oxygen ether groups, one or more amino ether groups, or both of one or more oxygen ether groups and one or more amino ether groups. Reaction of the oligomeric polyols with isocyanate monomers affords a new class of polyurethanes having superior heat and water resistance. The new polyurethanes exhibit lower peak exotherms, typically less than 250° F. during in-mold polymerization. Articles prepared from polyurethanes incorporating such oligomeric polyol compositions exhibit flexural strengths and moduli in excess of 10,000 psi and 400,000 psi respectively, and outstanding green strength.
-
公开(公告)号:US11072679B2
公开(公告)日:2021-07-27
申请号:US16105106
申请日:2018-08-20
申请人: Presidium USA, Inc
发明人: James Henry Blumsom , Andrew John Tennant , James A. Cella , David Goldwasser , Daniel J. Brunelle , Stephen Burks , Richard Heggs
IPC分类号: C08G59/62 , C08G18/40 , C08G18/48 , C08G18/46 , C08G18/50 , C08G18/44 , C08G18/42 , C08G18/76 , C08G64/42 , C08G18/32 , C08G18/02 , C08L75/04
摘要: There is provided an oligomeric polyol composition having (a) an oligomeric network containing residues of at least one polyhydroxylated aromatic compound and residues of at least one polyol having at least three hydroxyl groups; and (b) a plurality of peripheral groups having one or more pendant hydroxyl groups bound to the oligomeric network by a plurality of linking units. The residues of the polyol may optionally contain one or more oxygen ether groups, one or more amino ether groups, or both of one or more oxygen ether groups and one or more amino ether groups. Reaction of the oligomeric polyols with isocyanate monomers affords a new class of polyurethanes having superior heat and water resistance. The new polyurethanes exhibit lower peak exotherms, typically less than 250° F. during in-mold polymerization. Articles prepared from polyurethanes incorporating such oligomeric polyol compositions exhibit flexural strengths and moduli in excess of 10,000 psi and 400,000 psi respectively, and outstanding green strength.
-
公开(公告)号:US11066511B2
公开(公告)日:2021-07-20
申请号:US16105089
申请日:2018-08-20
申请人: Presidium USA, Inc
发明人: James Henry Blumsom , Andrew John Tennant , James A. Cella , David Goldwasser , Daniel J. Brunelle , Stephen Burks , Richard Heggs
IPC分类号: C08G59/62 , C08G18/40 , C08G18/48 , C08G18/46 , C08G18/50 , C08G18/44 , C08G18/42 , C08G18/76 , C08G64/42 , C08G18/32 , C08G18/02 , C08L75/04
摘要: There is provided an oligomeric polyol composition having (a) an oligomeric network containing residues of at least one polyhydroxylated aromatic compound and residues of at least one polyol having at least three hydroxyl groups; and (b) a plurality of peripheral groups having one or more pendant hydroxyl groups bound to the oligomeric network by a plurality of linking units. The residues of the polyol may optionally contain one or more oxygen ether groups, one or more amino ether groups, or both of one or more oxygen ether groups and one or more amino ether groups. Reaction of the oligomeric polyols with isocyanate monomers affords a new class of polyurethanes having superior heat and water resistance. The new polyurethanes exhibit lower peak exotherms, typically less than 250° F. during in-mold polymerization. Articles prepared from polyurethanes incorporating such oligomeric polyol compositions exhibit flexural strengths and moduli in excess of 10,000 psi and 400,000 psi respectively, and outstanding green strength.
-
公开(公告)号:US20190055346A1
公开(公告)日:2019-02-21
申请号:US16105148
申请日:2018-08-20
申请人: Presidium USA, Inc
发明人: James Henry Blumsom , Andrew John Tennant , James A. Cella , David Goldwasser , Daniel J. Brunelle , Stephen Burks , Richard Heggs
IPC分类号: C08G59/62 , C08G18/44 , C08G18/02 , C08G18/32 , C08G64/42 , C08G18/76 , C08G18/50 , C08G18/42 , C08G18/46 , C08G18/40 , C08G18/48 , C08L75/04
摘要: There is provided an oligomeric polyol composition having (a) an oligomeric network containing residues of at least one polyhydroxylated aromatic compound and residues of at least one polyol having at least three hydroxyl groups; and (b) a plurality of peripheral groups having one or more pendant hydroxyl groups bound to the oligomeric network by a plurality of linking units. The residues of the polyol may optionally contain one or more oxygen ether groups, one or more amino ether groups, or both of one or more oxygen ether groups and one or more amino ether groups. Reaction of the oligomeric polyols with isocyanate monomers affords a new class of polyurethanes having superior heat and water resistance. The new polyurethanes exhibit lower peak exotherms, typically less than 250° F. during in-mold polymerization. Articles prepared from polyurethanes incorporating such oligomeric polyol compositions exhibit flexural strengths and moduli in excess of 10,000 psi and 400,000 psi respectively, and outstanding green strength.
-
公开(公告)号:US20190040184A1
公开(公告)日:2019-02-07
申请号:US16105089
申请日:2018-08-20
申请人: Presidium USA, Inc
发明人: James Henry Blumson , Andrew John Tennant , James A. Cella , David Goldwasser , Daniel J. Brunelle , Stephen Burks , Richard Heggs
IPC分类号: C08G59/62 , C08G18/44 , C08G18/02 , C08G18/32 , C08G64/42 , C08G18/76 , C08G18/50 , C08G18/40 , C08G18/42 , C08G18/46 , C08G18/48 , C08L75/04
摘要: There is provided an oligomeric polyol composition having (a) an oligomeric network containing residues of at least one polyhydroxylated aromatic compound and residues of at least one polyol having at least three hydroxyl groups; and (b) a plurality of peripheral groups having one or more pendant hydroxyl groups bound to the oligomeric network by a plurality of linking units. The residues of the polyol may optionally contain one or more oxygen ether groups, one or more amino ether groups, or both of one or more oxygen ether groups and one or more amino ether groups. Reaction of the oligomeric polyols with isocyanate monomers affords a new class of polyurethanes having superior heat and water resistance. The new polyurethanes exhibit lower peak exotherms, typically less than 250° F. during in-mold polymerization. Articles prepared from polyurethanes incorporating such oligomeric polyol compositions exhibit flexural strengths and moduli in excess of 10,000 psi and 400,000 psi respectively, and outstanding green strength.
-
-
-
-
-
-
-
-
-