公开(公告)号:US20070286763A1
公开(公告)日:2007-12-13
申请号:US10590408
申请日:2005-03-31
CPC分类号: C22C21/00 , C22F1/04 , F28F21/084
摘要: The invention relates to a heat-resistant aluminium alloy for heat exchangers, a method for producing an aluminium strip or sheet for heat exchangers, and a corresponding aluminium strip or sheet. The aim of the invention is to provide an aluminium alloy and an aluminium strip or sheet which has a good recycling capacity, a Solidus temperature of at least 620° C., and an improved heat-resistance after welding. To this end, the inventive aluminium alloy comprises the following parts of alloy constituents in wL %: 0.3%≦Si≦1%, Fe≦0.5%, 0.3%≦Cu≦0.7%, 1.1%≦Mn≦1.8%, 0.15%≦Mg≦0.6%, 0.01%≦Cr≦0.3%, Zn≦0.10%, Ti≦0.3%, unavoidable impurities separately representing a maximum of 0.1%, and together a maximum of 0.15%, the remainder being aluminium.
摘要翻译: 本发明涉及一种用于热交换器的耐热铝合金,一种用于生产用于热交换器的铝带或片材的方法,以及相应的铝条或片材。 本发明的目的是提供一种铝合金和铝带或片,其具有良好的回收能力,至少620℃的固相线温度和焊接后的耐热性得到改善。 为此,本发明的铝合金包括以下组分:wL%:0.3%<= Si <= 1%,Fe <= 0.5%,0.3%<= Cu <= 0.7%,1.1%<= Mn <= 1.8%,0.15%<= Mg <= 0.6%,0.01%<= Cr <= 0.3%,Zn <= 0.10%,Ti <= 0.3%,不可避免的杂质分别代表最大0.1% 最大0.15%,其余为铝。
-
公开(公告)号:US06743396B2
公开(公告)日:2004-06-01
申请号:US10115712
申请日:2002-04-02
IPC分类号: C22C2116
CPC分类号: C22C21/00 , B32B15/016 , C22F1/04
摘要: The present invention relates to a method for producing AlMn strips or sheets for producing components by soldering, wherein a precursor material is produced from a melt which contains (in weight-percent) Si: 0.3-1.2%, Fe: ≦0.5%, Cu: ≦0.1%, Mn: 1.0-1.8%, Mg: ≦0.3%, Cr+Zr: 0.05-0.4%, Zn: ≦0.1% , Ti: ≦0.1% , Sn: ≦0.15%, and unavoidable companion elements, whose individual amounts are at most 0.05% and whose sum is at most 0.15%, as well as aluminum as the remainder, wherein the precursor material is preheated at a preheating temperature of less than 520° C. over a dwell time of at most 12 hours, wherein the preheated precursor material is hot rolled into a hot strip using a final hot rolling temperature of at least 250° C., wherein the hot strip is cold rolled into a cold strip without intermediate annealing.
摘要翻译: 本发明涉及一种用于通过焊接来生产组件的AlM薄带或片材的制造方法,其中前体材料由熔体制成,所述熔体含有(重量百分比)Si:0.3-1.2%,Fe:<= 0.5% Cu:<= 0.1%,Mn:1.0-1.8%,Mg:<= 0.3%,Cr + Zr:0.05-0.4%,Zn:<= 0.1%,Ti:≤0.1%,Sn: ,以及不可避免的伴随元素,其单独量为至多0.05%,其总和为0.15%以下,余量为铝,其中前体材料在小于520℃的预热温度下预热 停留时间至多12小时,其中使用最终热轧温度为至少250℃将预热的前体材料热轧成热带,其中将热带冷轧成冷带而不进行中间退火。
-