摘要:
The present invention provides a process of reducing the amount of fluorinated emulsifier in an aqueous fluoropolymer dispersion by contacting the aqueous fluoropolymer dispersion with an anion exchange resin in a non-fixed resin bed, the process comprising: (a) mixing the aqueous fluoropolymer dispersion with an effective amount of a surfactant so as to stabilize the fluoropolymer dispersion while being contacted with the anion exchange resin; (b) contacting the aqueous fluoropolyrner dispersion with an anion exchange resin by agitating the aqueous fluoropolymer dispersion with an effective amount of anion exchange resin for a time of less than 4 hours to reduce the amount of fluorinated emulsifier in the aqueous fluoropolymer dispersion to a desired level; and (c) separating the anion exchange resin from the aqueous fluoropolymer dispersion.
摘要:
The present invention provides a process of reducing the amount of fluorinated emulsifier in an aqueous fluoropolymer dispersion by contacting the aqueous fluoropolymer dispersion with an anion exchange resin in a non-fixed resin bed, the process comprising: (a) mixing the aqueous fluoropolymer dispersion with an effective amount of a surfactant so as to stabilize the fluoropolymer dispersion while being contacted with the anion exchange resin; (b) contacting the aqueous fluoropolymer dispersion with an anion exchange resin by agitating the aqueous fluoropolymer dispersion with an effective amount of anion exchange resin for a time of less than 4 hours to reduce the amount of fluorinated emulsifier in the aqueous fluoropolymer dispersion to a desired level; and (c) separating the anion exchange resin from the aqueous fluoropolymer dispersion.
摘要:
The present invention provides a fluoropolymer dispersion comprising fluoropolymer particles having an average particle size of 10 to 400 nm dispersed in water whereby the dispersion is free of fluorinated surfactant having a molecular weight of less than 1000 g/mol or contains the fluorinated surfactant having a molecular weight of less than 1000 g/mol in an amount of not more than 0.025% by weight based on the total weight of solids in the dispersion. The dispersion further comprises a non-ionic surfactant and an anionic surfactant selected from fluorinated anionic surfactants having a molecular weight of at least 1000 g/mol, non-fluorinated anionic surfactants and mixtures thereof.
摘要:
The present invention provides a fluoropolymer dispersion comprising fluoropolymer particles having an average particle size of 10 to 400 nm dispersed in water whereby the dispersion is free of fluorinated surfactant having a molecular weight of less than 1000 g/mol or contains the fluorinated surfactant having a molecular weight of less than 1000 g/mol in an amount of not more than 0.025% by weight based on the total weight of solids in the dispersion. The dispersion further comprises a non-ionic surfactant and an anionic surfactant selected from fluorinated anionic surfactants having a molecular weight of at least 1000 g/mol, non-fluorinated anionic surfactants and mixtures thereof.
摘要:
The present invention provides a fluoropolymer dispersion comprising fluoropolymer particles having an average particle size of 10 to 400 nm dispersed in water whereby the dispersion is free of fluorinated surfactant having a molecular weight of less than 1000 g/mol or contains the fluorinated surfactant having a molecular weight of less than 1000 g/mol in an amount of not more than 0.025% by weight based on the total weight of solids in the dispersion. The dispersion further comprises a non-ionic surfactant and an anionic surfactant selected from fluorinated anionic surfactants having a molecular weight of at least 1000 g/mol, non-fluorinated anionic surfactants and mixtures thereof.
摘要:
The present invention provides an aqueous fluoropolymer dispersion comprising a melt processible fluoropolymer in an amount of at least 25% by weight based on the weight of the aqueous fluoropolymer dispersion and a fluorinated surfactant having a molecular weight of not more than 1000 g/mol in an amount of not more than 100 ppm, preferably less than 50 ppm, more preferably less than 25 ppm and most preferably less than 10 ppm based on the weight of fluoropolymer solids or being free of said fluorinated surfactant. The aqueous fluoropolymer dispersion has a conductivity of at least 200 μS/cm, preferably at least 500 μS/cm and more preferably at least 1000 μS/cm.