Low burning rate, reduced hazard, high temperature incendiary
    1.
    发明授权
    Low burning rate, reduced hazard, high temperature incendiary 失效
    燃烧率低,危害低,燃烧温度高

    公开(公告)号:US06409854B1

    公开(公告)日:2002-06-25

    申请号:US09697246

    申请日:2000-10-27

    IPC分类号: C06B4510

    CPC分类号: C06B27/00

    摘要: A high temperature incendiary composition having a reactive material of titanium, a second reactive material of boron, an oxidizer of polytetrafluoroethylene in an amount of from about 10 weight percent or less of the composition and a binder of carboxyl-terminated polybutadiene acrylonitrile in an amount of from about 5 weight percent or more. The composition is safe to handle, ignites readily, burns at a low and controlled rate and produces a very high flame temperature.

    摘要翻译: 一种高温燃烧组合物,其具有钛的反应性材料,硼的第二反应性材料,聚四氟乙烯的氧化剂的量为组合物的约10重量%或更少,羧基封端的聚丁二烯丙烯腈的粘合剂的量为 约5重量%以上。 组合物易于处理,易燃点燃,以低和受控的速率燃烧并产生非常高的火焰温度。

    Lower burning rate, reduced hazard, high temperature incendiary
    2.
    发明授权
    Lower burning rate, reduced hazard, high temperature incendiary 失效
    降低燃烧率,降低危害,高温燃烧

    公开(公告)号:US06485586B1

    公开(公告)日:2002-11-26

    申请号:US09697252

    申请日:2000-10-27

    IPC分类号: C06B4510

    CPC分类号: C06C15/00 C06B27/00

    摘要: A low burning rate, high temperature incendiary composition having a reactive material of titanium, a second reactive material of boron, an oxidizer of polytetrafluoroethylene in an amount of from about 20 weight percent or greater of the composition and a binder of paraffin wax in an amount of from about 5 weight percent to about 20 weight percent. The composition is safe to handle, ignites readily, burns at a low and controlled rate and produces a very high flame temperature.

    摘要翻译: 具有钛的反应性材料的低燃烧速率,高温燃烧组合物,硼的第二反应性材料,聚四氟乙烯的氧化剂的量为组合物的约20重量%或更大,以及量的石蜡粘合剂 为约5重量%至约20重量%。 组合物易于处理,易燃点燃,以低和受控的速率燃烧并产生非常高的火焰温度。

    Low slag, reduced hazard, high temperature incendiary
    3.
    发明授权
    Low slag, reduced hazard, high temperature incendiary 失效
    炉渣低,危害小,耐高温燃烧

    公开(公告)号:US06402864B1

    公开(公告)日:2002-06-11

    申请号:US09697245

    申请日:2000-10-27

    IPC分类号: C06B4510

    CPC分类号: C06B27/00 C06B45/00 C06C15/00

    摘要: A high temperature incendiary composition having a reactive material of titanium, a second reactive material of boron, an oxidizer of polytetrafluoroethylene in an amount of from about 20 weight percent or greater of the composition and a binder of CTBN in an amount of from about 10 weight percent or less. The composition is safe to handle, ignites readily, produces low slag, burns at a low and controlled rate and produces a very high flame temperature.

    摘要翻译: 具有钛的反应性材料,硼的第二反应性材料,聚四氟乙烯的氧化剂的量为组合物的约20重量%或更高的高温燃烧组合物和CTBN的粘合剂,其量为约10重量% 百分之以内。 组合物易于处理,易点燃,产生低矿渣,以低和受控的速率燃烧并产生非常高的火焰温度。

    ESD sensitivity in titanium/boron compositions
    4.
    发明授权
    ESD sensitivity in titanium/boron compositions 失效
    钛/硼组成中的ESD敏感性

    公开(公告)号:US06723190B1

    公开(公告)日:2004-04-20

    申请号:US09697247

    申请日:2000-10-27

    IPC分类号: C06B4510

    CPC分类号: G06F13/1663

    摘要: A communication system comprises an input-output processor IOP (11) coupled to a plurality of network devices (10) and a protocol processor PP (12), both processors being coupled to a common memory (15). Memory access control means (16) resolves competition between the processors for memory access. Normally, if one of the two processors is accessing the memory, the memory control unit (16) allows that access to be completed before allowing the other processor to access the memory. But if data loss in a network device is imminent, the IOP, is granted a higher priority memory access, the memory access controller aborts (interrupts) any memory access by the PP, allowing the IOP to access the memory immediately.

    摘要翻译: 通过添加约5重量%以下的量的卵磷脂成分,提高具有钛反应性物质,硼的第二反应性物质和有效量的粘合剂的组合物中的ESD敏感性的方法。

    Melt cast thermoplastic elastomeric plastic bonded explosive
    6.
    发明授权
    Melt cast thermoplastic elastomeric plastic bonded explosive 失效
    熔体热塑性弹性塑料粘结炸药

    公开(公告)号:US4978482A

    公开(公告)日:1990-12-18

    申请号:US665906

    申请日:1984-10-29

    IPC分类号: C06B21/00

    CPC分类号: C06B21/005

    摘要: A method of melt casting plastic bonded explosives by:A. forming a uniform binder mixture of the following ingredients(1) from 10 to 30 weight percent of a triblock polymer of the formula A-B-A wherein A represents a polystyrene block and B represents an elastomeric midblock which is selected from the group consisting of polybutadiene, polyisoprene, and polyethylenebutylene; and(2) from 70 to 90 weight percent of a low viscosity oil selected from the group consisting of naphthenic, paraffinic, and olefinic oils by mixing the ingredients under low-shear conditions at a temperature of from 80.degree. C. to 110.degree. C.;B. mixing an energetic filler into the binder mixture under low shear conditions and at a temperature of from 80.degree. C. to 110.degree. C., provided that the viscosity of the mixture does not exceed 20 kilopoise;C. pouring the energetic filler-binder mixture formed in step B into a mold; andD. cooling energetic filler-binder mixture to form a solid explosive composite.Rubber phase associating and polystyrene phase associating hot melt resins may also be used in the binder mixture to improve the physical properties of the final plastic bonded explosive composite.

    摘要翻译: 一种通过以下方法熔融浇铸塑料粘结炸药的方法:A.形成以下成分(1)的均匀粘合剂混合物,10至30重量%的式ABA的三嵌段聚合物,其中A表示聚苯乙烯嵌段,B表示弹性体中间嵌段 其选自聚丁二烯,聚异戊二烯和聚乙烯丁烯; 和(2)70至90重量%的选自环烷烃,链烷烃和烯烃油的低粘度油,通过在低剪切条件下在80℃至110℃的温度下混合成分 。 B.在低剪切条件下和在80℃至110℃的温度下将能量填料混合到粘合剂混合物中,条件是混合物的粘度不超过20千泊; C.将步骤B中形成的高能填料 - 粘合剂混合物倒入模具中; 和D.冷却能量填料 - 粘合剂混合物以形成固体爆炸复合材料。 橡胶相缔合和聚苯乙烯相缔合的热熔树脂也可用于粘合剂混合物中以改善最终的塑料粘结的爆炸复合材料的物理性能。

    Process for the preparation of 2,4-dinitro-2,4-diazapentane
    7.
    发明授权
    Process for the preparation of 2,4-dinitro-2,4-diazapentane 失效
    2,4-二硝基-2,4-二氮杂戊烷的制备方法

    公开(公告)号:US4469888A

    公开(公告)日:1984-09-04

    申请号:US391902

    申请日:1982-06-25

    IPC分类号: C07C111/00

    CPC分类号: C07C241/00

    摘要: The invention is a process for reacting methylnitramine with formaldehyde a halogenated solvent and reacting the methylnitramine with formaldehyde in the presence of a strong sulfuric acid catalyst at certain specific temperatures to yield a final product having a yield rate of 70% or greater dimethylmethylenedinitraamine.

    摘要翻译: 本发明是一种使甲基硝基胺与甲醛在卤代溶剂中反应的方法,并在强硫酸催化剂存在下,在某些特定温度下使甲基硝基胺与甲醛反应,得到产率为70%或更高的二甲基亚甲基三胺的最终产物。

    New plasticizer for nitropolymers
    8.
    发明授权
    New plasticizer for nitropolymers 失效
    新型增塑剂用于硝基聚合物

    公开(公告)号:US4457791A

    公开(公告)日:1984-07-03

    申请号:US391901

    申请日:1982-06-25

    IPC分类号: C06B45/10

    CPC分类号: C06B45/105

    摘要: A novel composition of matter comprising a mixture of a nitrocellulose poer and a plasticizer comprising N,N' dimethyl methylene dinitramine.

    摘要翻译: 一种包含硝基纤维素聚合物和包含N,N'二甲基亚甲基二硝基胺的增塑剂的混合物的物质的新组合物。

    High energy explosives
    9.
    依法登记的发明
    High energy explosives 失效
    高能炸药

    公开(公告)号:USH1459H

    公开(公告)日:1995-07-04

    申请号:US233715

    申请日:1988-07-08

    IPC分类号: C06B45/10 C08G18/38 C08G18/56

    摘要: A high energy explosive composite which comprises(1) from about 2 to about 30 weight percent of an energetic polymer matrixf a urethane which is the reaction product of(a) a hydroxy-terminated prepolymer of the formula ##STR1## where R is --CH.sub.2 CF(NO.sub.2).sub.2 or --CH.sub.2 C(NO.sub.2).sub.2 CH.sub.3 ; A is --CH.sub.2 CH.sub.2, --CH.sub.2 OCH.sub.2 --, or --CH.sub.2 OCH.sub.2 OCH.sub.2 --, and n>1, and(b) a polyisocyanate which is used in an amount sufficient to supply from about 0.8:1 to about 1.5:1 isocyanate functional groups for each hydroxy functional group;(2) from about 8 to about 20 weight percent of an energetic plasticizer; and(3) from about 50 to about 90 weight percent of an explosive;wherein the energetic plasticizer and explosives are uniformly dispersed throughout the energetic polymer matrix.