摘要:
The present invention relates to a method of arranging and setting spray nozzles in a cooling apparatus comprising a plurality of pairs of constraining rolls for constraining and conveying a hot steel plate and one or more lines of spray nozzles between the pair of constraining rolls, each line having a plurality of spray nozzles and is disposed in a direction perpendicular to processing, and to the cooling apparatus and the method of cooling. The invention is characterized in that the spray nozzles are arranged such that a distribution of values ∫Pn between two edges of the steel plate in the direction perpendicular to processing is not less than 80% of its highest value, with P being cooling water impact pressure on the cooling surface, ∫Pn being the value of n power of P integrated in the processing direction between the pairs of constraining rolls, and 0.05≦n≦0.2.
摘要:
The present invention relates to an apparatus for cooling hot steel plate applied for controlled cooling of hot steel plate, obtained by hot rolling, while processing it constrained by constraining rolls and obtaining a steel material excellent and uniform in shape characteristics and provides a method of arranging and setting spray nozzles enabling uniform cooling in a direction perpendicular to processing and provides a method of arranging and setting spray nozzles of a spray cooling apparatus using two or more types of nozzles differing in amounts of water and spray regions to obtain a broad range of adjustment of amounts of water, wherein the spray nozzles are arranged so that a value of an n power of the impact pressures of the cooling water sprayed from the spray on the cooling surface integrated in the processing direction between pairs of constraining rolls becomes within −20% of the highest value in the direction perpendicular to processing, where, 0.05≦n≦0.2
摘要:
An apparatus for controlled cooling of hot steel plate while constraining and conveying the plate by constraining rolls horizontally which is inexpensive and enabling continuous control of the cooling ability over a broad range, that is, a cooling apparatus for spraying hot steel plate hot rolled and transferred between pairs of constraining rolls with cooling water from pluralities of lines of spray nozzles so as to cool the same, which apparatus has lines of gentle cooling spray nozzles and lines of strong cooling spray nozzles with different orifice shapes and enables continuous control of the cooling ability over a broad range due to the fact that a maximum cooling water impact pressure integrated value of the lines of gentle cooling spray nozzles and a minimum cooling water impact pressure integrated value of the lines of strong cooling spray nozzles are continuous.
摘要:
The present invention relates to an apparatus for cooling a hot steel plate which is processed and constrained by constraining rolls and a method of arranging and setting spray nozzles enabling uniform cooling in a direction perpendicular to processing. In the apparatus and method of the invention, the spray nozzles are arranged so that a value of n power of the impact pressure of the cooling water on the cooling surface integrated in the processing direction between pairs of constraining rolls becomes within −20% of the highest value in the direction perpendicular to processing, where 0.05≦n≦0.2.
摘要:
An apparatus for controlled cooling of hot steel plate while constraining and conveying the plate by constraining rolls horizontally which is inexpensive and enabling continuous control of the cooling ability over a broad range, that is, a cooling apparatus for spraying hot steel plate hot rolled and transferred between pairs of constraining rolls with cooling water from pluralities of lines of spray nozzles so as to cool the same, which apparatus has lines of gentle cooling spray nozzles and lines of strong cooling spray nozzles with different orifice shapes and enables continuous control of the cooling ability over a broad range due to the fact that a maximum cooling water impact pressure integrated value of the lines of gentle cooling spray nozzles and a minimum cooling water impact pressure integrated value of the lines of strong cooling spray nozzles are continuous.
摘要:
The present invention relates to an apparatus for cooling hot steel plate applied for controlled cooling of hot steel plate, obtained by hot rolling, while processing it constrained by constraining rolls and obtaining a steel material excellent and uniform in shape characteristics and provides a method of arranging and setting spray nozzles enabling uniform cooling in a direction perpendicular to processing and provides a method of arranging and setting spray nozzles of a spray cooling apparatus using two or more types of nozzles differing in amounts of water and spray regions to obtain a broad range of adjustment of amounts of water, wherein the spray nozzles are arranged so that a value of an n power of the impact pressures of the cooling water sprayed from the spray on the cooling surface integrated in the processing direction between pairs of constraining rolls becomes within −20% of the highest value in the direction perpendicular to processing, where, 0.05≦n≦0.2
摘要翻译:本发明涉及一种用于冷却热钢板的冷却装置,其通过热轧获得的热钢板的受控冷却,同时加工受到约束辊约束,并获得形状特性优良且均匀的钢材,并提供一种布置方法 并设置喷嘴,使得能够在垂直于加工的方向上均匀地冷却,并且提供了一种使用两种或多种不同水和喷射区域的喷嘴类型的喷嘴来布置和设置喷雾冷却装置的喷嘴的方法,以获得宽范围的调节 的水量,其中所述喷嘴被布置成使得从在所述约束辊对之间的处理方向上整合的冷却表面上的喷雾喷射的冷却水的冲击压力的n倍的值变为-20% 在垂直于加工的方向上具有最高值,其中,0.05 <= n <= 0.2
摘要:
A cooling method of a thick-gauge steel plate by spraying water from a plurality of spray nozzles on the top and bottom surfaces of the thick-gauge steel plate conveyed between the adjoining pairs of constraining rolls, each comprising a top roll and bottom roll, constraining and conveying the steel plate so as to efficiently cool the top and bottom surfaces of thick-gauge steel plate to secure symmetry of temperatures of the top and bottom surfaces and uniformity of temperature in the plate width direction and achieve improvement of flatness of thick-gauge steel plate and uniformity of quality.
摘要:
A cooling method of a thick-gauge steel plate by spraying water from a plurality of spray nozzles on the top and bottom surfaces of the thick-gauge steel plate conveyed between the adjoining pairs of constraining rolls, each comprising a top roll and bottom roll, constraining and conveying the steel plate so as to efficiently cool the top and bottom surfaces of thick-gauge steel plate to secure symmetry of temperatures of the top and bottom surfaces and uniformity of temperature in the plate width direction and achieve improvement of flatness of thick-gauge steel plate and uniformity of quality.
摘要:
The present invention provides a method of cooling a hot-rolled steel strip which has passed through a finishing rolling, including: cooling the hot-rolled steel strip from a first temperature of not lower than 600° C. and not higher than 650° C. to a second temperature of not higher than 450° C. with cooling water having the water amount density of not lower than 4 m3/m2/min and not higher than 10 m3/m2/min, wherein with respect to the area of the target surface, the area of a portion where a plurality of spray jets of the cooling water directly strikes on the target surface is at least 80%.
摘要翻译:本发明提供一种通过精轧的冷轧钢带的冷却方法,其特征在于,包括:从不低于600℃且不高于650℃的第一温度冷却所述热轧钢带 至不超过450℃的第二温度,其中水量密度不低于4m 3 / m 2 / min且不高于10m 3 / m 2 / min的冷却水,其中相对于 目标表面,冷却水的多个喷射射流直接撞击目标表面的部分的面积为至少80%。
摘要:
The present invention provides a method of cooling a hot-rolled steel strip which has passed through a finishing rolling, including: cooling the hot-rolled steel strip from a first temperature of not lower than 600° C. and not higher than 650° C. to a second temperature of not higher than 450° C. with cooling water having the water amount density of not lower than 4 m3/m2/min and not higher than 10 m3/m2/min, wherein with respect to the area of the target surface, the area of a portion where a plurality of spray jets of the cooling water directly strikes on the target surface is at least 80%.
摘要翻译:本发明提供一种通过精轧的冷轧钢带的冷却方法,其特征在于,包括:将所述热轧钢带从不低于600℃且不高于650℃的第一温度冷却 至不超过450℃的第二温度,其中水量密度不低于4m 3 / m 2 / min且不高于10m 3 / m 2 / min的冷却水,其中相对于 目标表面,冷却水的多个喷射射流直接撞击目标表面的部分的面积为至少80%。