NEGATIVE ELECTRODE FOR LITHIUM SECONDARY BATTERY AND LITHIUM SECONDARY BATTERY COMPRISING SAME

    公开(公告)号:US20230028390A1

    公开(公告)日:2023-01-26

    申请号:US17930714

    申请日:2022-09-08

    Abstract: A negative electrode for a lithium secondary battery comprises a current collector and a negative electrode active material layer formed on the current collector, wherein the negative electrode active material layer includes a first negative electrode active material and a first binder, and a second active material layer formed on the first active material layer and including a second negative electrode active material and a second binder, a content of the first binder is greater than that of the second binder, a loading level of the negative electrode active material layer is 10 mg/cm2 to 30 mg/cm2, a loading level of the first active material layer is 4 mg/cm2 to 25 mg/cm2, a loading level of the second active material layer is 4 mg/cm2 to 25 mg/cm2, and a loading level of the second active material layer is equal to or higher than that of the first active material layer.

    NEGATIVE ELECTRODE FOR LITHIUM SECONDARY BATTERY AND LITHIUM SECONDARY BATTERY COMPRISING SAME

    公开(公告)号:US20230017229A1

    公开(公告)日:2023-01-19

    申请号:US17930715

    申请日:2022-09-08

    Abstract: A negative electrode for a lithium secondary battery comprises a current collector and a negative electrode active material layer formed on the current collector, wherein the negative electrode active material layer includes a first negative electrode active material and a first binder, and a second active material layer formed on the first active material layer and including a second negative electrode active material and a second binder, a content of the first binder is greater than that of the second binder, a loading level of the negative electrode active material layer is 10 mg/cm2 to 30 mg/cm2, a loading level of the first active material layer is 4 mg/cm2 to 25 mg/cm2, a loading level of the second active material layer is 4 mg/cm2 to 25 mg/cm2, and a loading level of the second active material layer is equal to or higher than that of the first active material layer.

    NEGATIVE ELECTRODE FOR LITHIUM SECONDARY BATTERY AND LITHIUM SECONDARY BATTERY COMPRISING SAME

    公开(公告)号:US20230006212A1

    公开(公告)日:2023-01-05

    申请号:US17930676

    申请日:2022-09-08

    Abstract: The present invention relates to a negative electrode for a lithium secondary battery and a lithium secondary battery comprising the same. The negative electrode for a lithium secondary battery comprises a current collector and a negative electrode active material layer formed on the current collector, wherein the negative electrode active material layer includes a first negative electrode active material and a first binder, and a second active material layer formed on the first active material layer and including a second negative electrode active material and a second binder, a content of the first binder is greater than that of the second binder, a loading level of the negative electrode active material layer is 10 mg/cm2 to 30 mg/cm2, a loading level of the first active material layer is 4 mg/cm2 to 25 mg/cm2, a loading level of the second active material layer is 4 mg/cm2 to 25 mg/cm2, and a loading level of the second active material layer is equal to or higher than that of the first active material layer.

    NEGATIVE ELECTRODE FOR LITHIUM SECONDARY BATTERY AND LITHIUM SECONDARY BATTERY COMPRISING SAME

    公开(公告)号:US20200335795A1

    公开(公告)日:2020-10-22

    申请号:US16753319

    申请日:2018-08-27

    Abstract: The present invention relates to a negative electrode for a lithium secondary battery and a lithium secondary battery comprising the same. The negative electrode for a lithium secondary battery comprises a current collector and a negative electrode active material layer formed on the current collector, wherein the negative electrode active material layer includes a first negative electrode active material and a first binder, and a second active material layer formed on the first active material layer and including a second negative electrode active material and a second binder, a content of the first binder is greater than that of the second binder, a loading level of the negative electrode active material layer is 10 mg/cm2 to 30 mg/cm2, a loading level of the first active material layer is 4 mg/cm2 to 25 mg/cm2, a loading level of the second active material layer is 4 mg/cm2 to 25 mg/cm2, and a loading level of the second active material layer is equal to or higher than that of the first active material layer.