NEGATIVE ELECTRODE FOR LITHIUM SECONDARY BATTERY AND LITHIUM SECONDARY BATTERY COMPRISING SAME

    公开(公告)号:US20230028390A1

    公开(公告)日:2023-01-26

    申请号:US17930714

    申请日:2022-09-08

    Abstract: A negative electrode for a lithium secondary battery comprises a current collector and a negative electrode active material layer formed on the current collector, wherein the negative electrode active material layer includes a first negative electrode active material and a first binder, and a second active material layer formed on the first active material layer and including a second negative electrode active material and a second binder, a content of the first binder is greater than that of the second binder, a loading level of the negative electrode active material layer is 10 mg/cm2 to 30 mg/cm2, a loading level of the first active material layer is 4 mg/cm2 to 25 mg/cm2, a loading level of the second active material layer is 4 mg/cm2 to 25 mg/cm2, and a loading level of the second active material layer is equal to or higher than that of the first active material layer.

    NEGATIVE ELECTRODE FOR LITHIUM SECONDARY BATTERY AND LITHIUM SECONDARY BATTERY COMPRISING SAME

    公开(公告)号:US20200335795A1

    公开(公告)日:2020-10-22

    申请号:US16753319

    申请日:2018-08-27

    Abstract: The present invention relates to a negative electrode for a lithium secondary battery and a lithium secondary battery comprising the same. The negative electrode for a lithium secondary battery comprises a current collector and a negative electrode active material layer formed on the current collector, wherein the negative electrode active material layer includes a first negative electrode active material and a first binder, and a second active material layer formed on the first active material layer and including a second negative electrode active material and a second binder, a content of the first binder is greater than that of the second binder, a loading level of the negative electrode active material layer is 10 mg/cm2 to 30 mg/cm2, a loading level of the first active material layer is 4 mg/cm2 to 25 mg/cm2, a loading level of the second active material layer is 4 mg/cm2 to 25 mg/cm2, and a loading level of the second active material layer is equal to or higher than that of the first active material layer.

    ELECTRODE AND RECHARGEABLE LITHIUM BATTERY INCLUDING THE SAME

    公开(公告)号:US20230246200A1

    公开(公告)日:2023-08-03

    申请号:US18159048

    申请日:2023-01-24

    CPC classification number: H01M4/667 H01M4/623

    Abstract: An electrode including a current collector; an electrode active material layer on a surface of the current collector and including internal pores; an inner coating layer filled in the internal pores of the electrode active material layer and including an adhesive material; and an outer coating layer disposed on a surface of the electrode active material layer and including an adhesive material. A total weight of the inner coating layer and the outer coating layer per area of one surface of the current collector is about 0.1 g/m2 to about 0.7 g/m2. In addition, the electrode active material layer has a porosity of about 13% to about 16% in a cross section having a depth of about 20 μm from the surface of the electrode active material layer to the current collector.