公开(公告)号:US10364184B2
公开(公告)日:2019-07-30
申请号:US15749780
申请日:2017-02-14
Applicant: SOUTHWEST PETROLEUM UNIVERSITY
Inventor: Ping Guo , Shuai Wu , Yijian Chen , Huimin Zhang , Wanbo Zhang , Yuhong Du , Zhouhua Wang , Jianfen Du , Yisheng Hu , Huang Liu , Hongmei Ren
IPC: C04B20/10 , C04B28/04 , C04B14/04 , C04B40/00 , G01N1/28 , C04B14/06 , B28B7/38 , C04B111/00 , C09K8/46
Abstract: A manufacturing method of a big-model low-permeability microcrack core includes: (1) determining the size of a microcrack core to be manufactured; (2) placing stones in a baking oven to bake for 24h under 120° C., placing the stones into a mixer, mixing and spraying oil, enabling the oil to seep into the stone, evenly forming a thin oil film on stone's surface; (3) mixing the oil sprayed stone with quartz sand and cement, adding water to mix evenly to obtain cement paste; (4) spreading butter on core mold's inner surface to form a thin butter film, pouring the cement paste into the core mold to obtain a cement sample; (5) loading confining pressure outside the core according to the requirements of porosity and permeability of the mold to adjust a pore permeability value; (6) obtaining the big-model core with microcrack after the cement sample is dried and formed.