Abstract:
Provided is a method for making a supported metal catalyst. The method includes forming a mixture comprising a high surface area support, a reducing agent precursor that decomposes to produce reducing gases below about 1200° C., and a metal catalyst precursor. The mixture is heated to a temperature sufficient to decompose the reducing agent precursor to produce a reducing agent, and then cooled to form the supported metal catalyst.