CARBURIZED PART, METHOD FOR MANUFACTURING THEREOF, AND STEEL FOR CARBURIZED PART
    1.
    发明申请
    CARBURIZED PART, METHOD FOR MANUFACTURING THEREOF, AND STEEL FOR CARBURIZED PART 有权
    加工部件,其制造方法和加固部件的钢

    公开(公告)号:US20140299234A1

    公开(公告)日:2014-10-09

    申请号:US14245229

    申请日:2014-04-04

    IPC分类号: C23C8/22 C23C8/02

    CPC分类号: C23C8/22 C23C8/02 C23C8/80

    摘要: The invention provides a carburized part which has excellent medium-cycle fatigue strength in particular subjected to surface-hardening treatment by carburization. The invention provides a carburized part including a carburized layer formed by performing carburizing treatment to a steel, the steel including, in terms of % by mass: 0.15% to 0.25% of C, 0.15% or less of Si, 0.4% to 1.1% of Mn, 0.8% to 1.4% of Cr, 0.25% to 0.55% of Mo, 0.015% or less of P, and 0.035% or less of S, with the remainder being Fe and unavoidable impurities, and the steel satisfying the following relation; 0.10≦[Mo]/(10[Si]+[Mn]+[Cr])≦0.40, in which [M] represents a content of element M in terms of % by mass.

    摘要翻译: 本发明提供一种具有优异的中等循环疲劳强度的渗碳部件,特别是通过渗碳进行表面硬化处理。 本发明提供一种渗碳部分,其包括通过对钢进行渗碳处理而形成的渗碳层,所述钢以质量%计含有:0.15〜0.25%的C,0.15%以下的Si,0.4〜1.1% 的Mn,0.8〜1.4%的Cr,0.25〜0.55%的Mo,0.015%以下的P和0.035%以下的S,余量为Fe和不可避免的杂质,满足以下关系的钢 ; 0.10≦̸ [Mo] /(10 [Si] + [Mn] + [Cr])≦̸ 0.40,其中[M]表示元素M的含量,以质量%计。