摘要: A process for producing a polybutadiene is provided wherein, first, 1,3-butadiene is polymerized in the presence of a particular cis-1,4-polymerization catalyst and subsequently, the polymerization is continued in the presence of a particular 1,2-polymerization catalyst. The resulting polybutadiene is characterized as containing 2 to 40% of the 1,2-structure, the melting point of the 1,2-structure portion being 110.degree. to 215.degree.C, and containing 60 to 98% of the cis-1,4-structure and having an intrinsic viscosity [.eta.] of 0.9 to 8 in tetraline at 135.degree.C. A vulcanized product of the polybutadiene is characterized as possessing improved tear strength, flex-crack resistance and tensile strength.
摘要翻译: 提供一种生产聚丁二烯的方法,其中首先在特定的顺式-1,4-聚合催化剂存在下聚合1,3-丁二烯,随后在特定的1,2- 聚合催化剂。 所得聚丁二烯的特征在于含有2〜40%的1,2-结构,1,2-结构部分的熔点为110〜215℃,含有60〜98%的顺式-1, 4-结构,在135℃下在四氢化萘中的特性粘度η为0.9-8。聚丁二烯的硫化产物的特征在于具有改善的撕裂强度,抗弯曲性和拉伸强度。