Storage-stable modified asphalt composition and its preparation process
    1.
    发明授权
    Storage-stable modified asphalt composition and its preparation process 有权
    储存稳定改性沥青组合物及其制备方法

    公开(公告)号:US06713539B2

    公开(公告)日:2004-03-30

    申请号:US09931846

    申请日:2001-08-17

    IPC分类号: C08L9500

    摘要: A storage-stable modified asphalt composition, which comprises: 50-97.7 parts by weight of a base asphalt, 2.0-20.0 parts by weight of a polymer having double bonds, 0.1-20.0 parts by weight of a compatibilizer, 0.1-10.0 parts by weight of a cross-linking reagent, and 0.1-10.0 parts by weight of a organic polar compound, and the softening point difference of its product determined by the stability test is lower than 2.5° C. The process for preparing said modified asphalt composition is mixing 50-97.7 parts by weight of a base asphalt, 2.0-20.0 parts by weight of a polymer having double bonds, 0.1-20.0 parts by weight of a compatibilizer 0.1-10.0 parts by weight of a cross-linking reagent, and 0.1-10.0 parts by weight of a organic polar compound under certain conditions. The modified asphalt provided by the present invention has good storage-stability. The preparation process provided by the present invention is simple, and there is no need for special apparatus.

    摘要翻译: 一种储存稳定的改性沥青组合物,其包含:50-97.7重量份的基础沥青,2.0-20.0重量份的具有双键的聚合物,0.1-20.0重量份增容剂,0.1-10.0重量份 交联剂的重量和0.1-10.0重量份的有机极性化合物,并且通过稳定性试验测定的其产物的软化点差低于2.5℃。制备所述改性沥青组合物的方法是 混合50-97.7重量份的基础沥青,2.0-20.0重量份的具有双键的聚合物,0.1-20.0重量份增容剂0.1-10.0重量份的交联剂和0.1- 10.0份(重量)有机极性化合物。 由本发明提供的改性沥青具有良好的储存稳定性。 本发明提供的制备方法简单,不需要特殊的装置。