Storage-stable modified asphalt composition and its preparation process
    1.
    发明授权
    Storage-stable modified asphalt composition and its preparation process 有权
    储存稳定改性沥青组合物及其制备方法

    公开(公告)号:US06713539B2

    公开(公告)日:2004-03-30

    申请号:US09931846

    申请日:2001-08-17

    IPC分类号: C08L9500

    摘要: A storage-stable modified asphalt composition, which comprises: 50-97.7 parts by weight of a base asphalt, 2.0-20.0 parts by weight of a polymer having double bonds, 0.1-20.0 parts by weight of a compatibilizer, 0.1-10.0 parts by weight of a cross-linking reagent, and 0.1-10.0 parts by weight of a organic polar compound, and the softening point difference of its product determined by the stability test is lower than 2.5° C. The process for preparing said modified asphalt composition is mixing 50-97.7 parts by weight of a base asphalt, 2.0-20.0 parts by weight of a polymer having double bonds, 0.1-20.0 parts by weight of a compatibilizer 0.1-10.0 parts by weight of a cross-linking reagent, and 0.1-10.0 parts by weight of a organic polar compound under certain conditions. The modified asphalt provided by the present invention has good storage-stability. The preparation process provided by the present invention is simple, and there is no need for special apparatus.

    摘要翻译: 一种储存稳定的改性沥青组合物,其包含:50-97.7重量份的基础沥青,2.0-20.0重量份的具有双键的聚合物,0.1-20.0重量份增容剂,0.1-10.0重量份 交联剂的重量和0.1-10.0重量份的有机极性化合物,并且通过稳定性试验测定的其产物的软化点差低于2.5℃。制备所述改性沥青组合物的方法是 混合50-97.7重量份的基础沥青,2.0-20.0重量份的具有双键的聚合物,0.1-20.0重量份增容剂0.1-10.0重量份的交联剂和0.1- 10.0份(重量)有机极性化合物。 由本发明提供的改性沥青具有良好的储存稳定性。 本发明提供的制备方法简单,不需要特殊的装置。

    Combined process of low degree solvent deasphalting and delayed coking
    2.
    发明授权
    Combined process of low degree solvent deasphalting and delayed coking 有权
    低溶剂脱沥青和延迟焦化的联合工艺

    公开(公告)号:US06673234B2

    公开(公告)日:2004-01-06

    申请号:US09965601

    申请日:2001-09-25

    IPC分类号: C10C300

    CPC分类号: C10G55/04

    摘要: A combined process of low degree solvent deasphalting and delayed coking, which comprises feeding a deasphalting stock and a solvent into an extractor and making the yield of the deasphalted oil 70 wt %-95 wt %, and introducing a part or all of the deasphalted oil and optionally a conventional coking stock into a delayed coker. This process increases the yield of liquid products, removes the heavy asphaltene which is prone to coke, extends the run length of the delayed coker, and at the same time, lowers the content of impurities in coke, enlarges the sources of the stocks for producing the needle coke.

    摘要翻译: 低度溶剂脱沥青和延迟焦化的组合方法,其包括将脱沥青原料和溶剂进料到萃取器中,使脱沥青油的产率为70重量%-95重量%,并将部分或全部脱沥青油 和任选的常规焦化原料进入延迟焦化器。 这个过程增加了液体产品的产量,去除易于焦炭的重质沥青质,延长了焦化炉的运行时间,同时降低了焦炭中的杂质含量,从而扩大了生产原料的来源 针状焦炭。