摘要: The present invention herein provides silica powder which can be incorporated into a sealing material at a high content to thus give a sealing material having excellent moldability. The silica powder at least has, in the volume-based frequency distribution of particle size as determined by the laser diffraction-scattering technique, a maximum frequency value for a mode peak 1 present in a particle size range extending from 1 to 4 μm and a maximum frequency value for a mode peak 2 present in a particle size range extending from 15 to 55 μm, wherein the maximum frequency value for the mode peak 2 is greater than that for the mode peak 1, the mode peak 2 has a shoulder, and the content of particles whose particle size ranges from 15 to 55 μm is larger than that of particles whose particle size ranges from 1 to 4 μm.
摘要翻译: 本发明提供二氧化硅粉末,其可以以高含量掺入到密封材料中,从而得到具有优异成型性的密封材料。 二氧化硅粉末在通过激光衍射 - 散射技术确定的基于体积的粒径频率分布中至少具有存在于从1至4μm的粒度范围内存在的模式峰1的最大频率值和 存在于15〜55μm的粒度范围内的模式峰值2的最大频率值,其中模式峰值2的最大频率值大于模式峰值1的最大频率值,模式峰值2具有肩部,并且 粒度为15〜55μm的粒子的含量比粒径为1〜4μm的粒子的含量大。
-
公开(公告)号:US07820750B2
公开(公告)日:2010-10-26
申请号:US12091998
申请日:2007-03-19
申请人: Shuji Sasaki , Norihisa Nakashima
发明人: Shuji Sasaki , Norihisa Nakashima
CPC分类号: H01L23/295 , C01B33/18 , C01P2002/70 , C01P2004/61 , C04B14/06 , C04B20/008 , C09C1/30 , H01L2924/0002 , H01L2924/00
摘要: The present invention herein provides silica powder which can be incorporated into a sealing material at a high content to thus give a sealing material having excellent moldability. The silica powder at least has, in the volume-based frequency distribution of particle size as determined by the laser diffraction-scattering technique, a maximum frequency value for a mode peak 1present in a particle size range extending from 1 to 4 μm and a maximum frequency value for a mode peak 2 present in a particle size range extending from 15 to 55 μm, wherein the maximum frequency value for the mode peak 2 is greater than that for the mode peak 1, the mode peak 2 has a shoulder, and the content of particles whose particle size ranges from 15 to 55 μm is larger than that of particles whose particle size ranges from 1 to 4 μm.
摘要翻译: 本发明提供二氧化硅粉末,其可以以高含量掺入密封材料中,从而得到具有优异成型性的密封材料。 二氧化硅粉末在通过激光衍射 - 散射技术确定的基于体积的粒径频率分布中至少具有在1至4μm范围内延伸的粒度范围内的模式峰1的最大频率值和最大值 存在于从15至55μm的粒度范围内的模式峰值2的频率值,其中模式峰值2的最大频率值大于模式峰值1的最大频率值,模式峰值2具有肩部,并且 粒径为15〜55μm的粒子的粒径大于粒径为1〜4μm的粒子的含量。
-
公开(公告)号:US6054073A
公开(公告)日:2000-04-25
申请号:US138567
申请日:1998-08-24
IPC分类号: B01J2/16 , B01J2/00 , C01B13/14 , C01B33/12 , C01B33/18 , C01B33/26 , C01F7/02 , C01F7/16 , C03B8/04 , C03B19/10 , C03B20/00 , C04B35/14 , C04B35/18 , C04B35/185 , C04B35/443 , C04B35/622 , C04B35/64 , B22D11/01
CPC分类号: C04B35/622 , B01J2/00 , C01B33/12 , C01B33/26 , C01F7/027 , C01F7/162 , C03B19/1025 , C04B35/14 , C04B35/18 , C04B35/185 , C04B35/443 , C04B35/64 , C01P2004/32 , C01P2004/61 , C01P2004/62
摘要: An apparatus for producing inorganic spherical particles by supplying raw material through a burner so as to pass through a flame and injecting it into a cooling tower, characterized in that the inner surface of the cooling tower is made of a metal.
摘要翻译: 一种生产无机球形颗粒的装置,其通过燃烧器供应原料以便通过火焰并将其注入冷却塔中,其特征在于冷却塔的内表面由金属制成。
-
-