摘要:
A separable distribution rotor and a horizontal rotor distributor having the same. The separable distribution rotor includes a first distribution rotor, a second distribution rotor, and an elastic member interposed between the first distribution rotor and the second distribution rotor.
摘要:
A separable distribution rotor and a horizontal rotor distributor having the same. The separable distribution rotor includes a first distribution rotor, a second distribution rotor, and an elastic member interposed between the first distribution rotor and the second distribution rotor.
摘要:
Provided are a bake hardening steel having a crystalline grain size of ASTM No. 9 or more and a method for preparing the bake hardening steel by controlling the winding, rolling and cooling conditions. The bake hardening steel includes: C:0.0016˜0.0025%, Si:0.02% or less, P:0.01˜0.05%, S:0.01% or less, sol.Al:0.08˜0.12%, N:0.0025% or less, Ti:0.003% or less, Nb:0.003˜0.011%, Mo:0.01˜0.1%, B:0.0005˜0.0015% or less, balance Fe and other inevitable impurities, wherein % is weight %, and Mn and P satisfy the relation of −30(° C.)≧803P−24.4Mn−58.
摘要:
Disclosed herein are a bake-hardenable high-strength cold-rolled steel sheet, a hot-dipped steel sheet thereof, and a method for manufacturing the same. The steel sheet comprises 0.0016˜0.01% of C; 0.1% or less of Si; 0.2˜1.5% of Mn; 0.05˜0.15% of P; 0.01% or less of S; 0.08˜0.5% of (soluble) Al; 0.0025% or less of N; 0.003˜0.1% of Nb; 0.003% of less of Ti; 0.01˜0.4% of Mo; 0.0005˜0.005% of B; and the balance of Fe and other unavoidable impurities, in terms of weight %. The steel sheet has fine AlN precipitates, and a grain size (ASTM No.) of 9 or more. The AlN precipitates have a grain size, which can suppress grain growth. The steel sheet has enhanced strength, bake hardenability, aging resistance, and secondary work embrittlement resistance.
摘要:
It is an object of the present invention to provide a high strength cold-rolled steel sheet, which has superior bake hardenability, aging resistance at room temperature and secondary work embrittlement resistance, and a method for manufacturing the same. The steel sheet has a grain size of ASTM No. of 9 or more after annealing, a BH of 30 MPa or more, an AI of 30 MPa or less, and a tensile strength of 340˜390 MPa through appropriate control of solute elements in steel by addition of a small amount of Ti, addition of Al and Mo, and control of manufacturing conditions, and refinement of crystal grains after annealing. The cold-rolled steel sheet and the galvannealed steel sheet produced using the cold-rolled steel sheet have the superior bake hardenability, aging resistance at room temperature, and secondary work embrittlement resistance.
摘要:
A cold-rolled steel sheet for outer panels and the like of an automobile body, a galvannealed steel sheet using the cold-rolled steel sheet, and a method for manufacturing the same are disclosed. It is an object of the present invention to provide a high strength cold-rolled steel sheet, which has superior bake hardenability, aging resistance at room temperature and secondary work embrittlement resistance, and a method for manufacturing the same. The steel sheet has a grain size of ASTM No. of 9 or more after annealing, a BH of 30 MPa or more, an AI of 30 MPa or less, and a tensile strength of 340˜390 MPa through appropriate control of solute elements in steel by addition of a small amount of Ti, addition of Al and Mo, and control of manufacturing conditions, and refinement of crystal grains after annealing. The cold-rolled steel sheet and the galvannealed steel sheet produced using the cold-rolled steel sheet have the superior bake hardenability, aging resistance at room temperature, and secondary work embrittlement resistance.
摘要:
A bake-hardenable high-strength cold-rolled steel sheet, a hot-dipped steel sheet thereof, and a method for manufacturing the same. The steel sheet comprises 0.0016˜0.01% of C; 0.1% or less of Si; 0.2˜1.5% of Mn; 0.05˜0.15% of P; 0.01% or less of S; 0.08˜0.5% of (soluble) Al; 0.0025% or less of N; 0.003˜0.1% of Nb; 0.003% or less of Ti; 0.01˜0.4% of Mo; 0.0005˜0.005% of B; and the balance of Fe and other unavoidable impurities, in terms of weight %. The method includes the steps of heating a steel slab of the above composition to a temperature of 1,200° C. or more; and then hot rolling the steel slab with finish rolling at or above the Ar3 temperature to provide a hot rolled steel sheet; coiling the hot rolled steel sheet; cold rolling the hot rolled and coiled sheet; and continuous annealing the cold rolled sheet.
摘要:
A bake-hardenable cold rolled steel sheet with high strength and superior aging resistance used for outer panels of an automobile body, a galvannealed steel sheet using the cold-rolled steel sheet, and a method for manufacturing the cold-rolled steel sheet are disclosed. The steel sheet comprises, by weight %, C: 0.0016˜0.0025%, Si: 0.02% or less, Mn: 0.2˜1.2%, P: 0.05˜0.11%, S: 0.01% or less, Sol. Al: 0.08˜0.12%, N: 0.0025% or less, Ti: 0˜0.003%, Nb: 0.003˜0.011%, Mo: 0.01˜0.1%, B: 0.0005˜0.0015%, the balance of Fe and other unavoidable impurities. The steel sheet has superior bake hardenability, aging resistance at room temperature, and secondary work embrittlement resistance.
摘要:
Provided are a bake hardening steel having a crystalline grain size of ASTM No. 9 or more and a method for preparing the bake hardening steel by controlling the winding, rolling and cooling conditions. The bake hardening steel includes: C:0.0016˜0.0025%, Si:0.02% or less, P:0.01˜0.05%, S:0.01% or less, sol.Al:0.08˜0.12%, N:0.0025% or less, Ti:0.003% or less, Nb:0.003˜0.011%, Mo:0.01˜0.1%, B:0.0005˜0.0015% or less, balance Fe and other inevitable impurities, wherein % is weight %, and Mn and P satisfy the relation of −30(° C.)≧803P−24.4Mn−58.
摘要:
A cold-rolled steel sheet for outer panels and the like of an automobile body, a galvannealed steel sheet using the cold-rolled steel sheet, and a method for manufacturing the same are disclosed. It is an object of the present invention to provide a high strength cold-rolled steel sheet, which has superior bake hardenability, aging resistance at room temperature and secondary work embrittlement resistance, and a method for manufacturing the same. The steel sheet has a grain size of ASTM No. of 9 or more after annealing, a BH of 30 MPa or more, an AI of 30 MPa or less, and a tensile strength of 340˜390 MPa through appropriate control of solute elements in steel by addition of a small amount of Ti, addition of Al and Mo, and control of manufacturing conditions, and refinement of crystal grains after annealing. The cold-rolled steel sheet and the galvannealed steel sheet produced using the cold-rolled steel sheet have the superior bake hardenability, aging resistance at room temperature, and secondary work embrittlement resistance.