公开(公告)号:US06640462B1
公开(公告)日:2003-11-04
申请号:US10030107
申请日:2002-05-30
申请人: Sun Tae Choi , Vladimir Petrovich Golitsyn , Natalya Vladimirovna Golitsyna , Nam Joo Huh , Kun Pyo Kim
发明人: Sun Tae Choi , Vladimir Petrovich Golitsyn , Natalya Vladimirovna Golitsyna , Nam Joo Huh , Kun Pyo Kim
IPC分类号: F26B700
CPC分类号: F26B5/04 , F26B21/10 , F26B2210/16
摘要: Disclosed is a method of drying timbers loaded in a drying chamber, which comprises the steps of heating the drying chamber by a heating system up to a temperature of 80 to 100° C., subjecting the timbers to vacuum blowing by connecting the inside of the drying chamber with a vacuum chamber (receiver) evacuated by a rotary pump until the inside pressure of the drying chamber drops to 1 to 10 mmHg, disconnecting the inside of the drying chamber from the vacuum chamber, connecting the drying chamber with the atmosphere. When the inside of the drying chamber is connected with the vacuum chamber, the moisture content of the timbers is sharply reduced, so that their temperature sharply drops. Thereafter, when it is disconnected from the vacuum chamber, and connected with the atmosphere, the inside temperature of the drying chamber is again increased. Meanwhile, the heating system is worked during the whole process. The above steps constitute one cycle that is sequentially repeated until the moisture content of the timbers drops to a desired level. Preferably, the connection between the drying chamber with the vacuum chamber is made in 0.1 to 0.5 seconds. Pressure release is made in the vacuum for 0.5 to 5.0 seconds until reaching equilibrium moisture. The blow-down in the vacuum is carried out by a heat carrier with a temperature of 80 to 150° C. until reaching the volume average material temperature of 80 to 90° C. with the subsequent pressure release in the drying chamber lower than the equilibrium, thus providing high-speed vacuum blowing.
摘要翻译: 本发明公开了一种干燥室中装载的木材的方法,其特征在于包括以下步骤:通过加热系统将干燥室加热到80-100℃的温度,通过将木材的内部连接 干燥室具有通过旋转泵抽真空的真空室(接收器),直到干燥室的内部压力下降到1至10mmHg,将干燥室的内部与真空室断开,将干燥室与大气连接。 当干燥室的内部与真空室连接时,木材的含水量急剧降低,使得它们的温度急剧下降。 此后,当与真空室断开并与大气连接时,干燥室的内部温度再次增加。 同时,加热系统在整个过程中工作。 上述步骤构成一个循环,其顺序重复,直到木材的水分含量降至期望水平。 优选地,干燥室与真空室之间的连接在0.1至0.5秒内进行。 压力释放在真空中进行0.5至5.0秒,直到达到平衡水分。 真空中的吹扫由温度为80-150℃的载热体进行,直到达到体积平均材料温度为80至90℃,随后干燥室中的压力释放低于 平衡,从而提供高速真空吹风。