Boiler tube having improved high temperature mechanical strength,
improved high temperature corrosion resistant property and resistance
to embrittlement during service
    2.
    发明授权
    Boiler tube having improved high temperature mechanical strength, improved high temperature corrosion resistant property and resistance to embrittlement during service 失效
    锅炉管具有改善的高温机械强度,改善的高温耐腐蚀性能和在使用过程中的脆化性

    公开(公告)号:US4463061A

    公开(公告)日:1984-07-31

    申请号:US502836

    申请日:1983-06-09

    摘要: A boiler tube having improved high temperature strength, improved high temperature corrosion resistance, and resistivity to embrittlement during the service thereof, comprising an outer surface layer and an inner part, the outer surface layer consisting essentially, by weight, of 0.03-0.20% carbon, 1.5-4.0% silicon, 0.1-3.0% manganese, 13-25% chromium, 13-40% nickel, 0.5-3.0% at least one kind selected from the group consisting of molybdenum and tungsten, 0.05-0.5% at least one kind selected from the group consisting of titanium, niobium and vanadium, and the balance iron and inevitable impurities, the inner part consisting essentially, by weight, of 0.03-0.20% carbon, 0.3-1.0% silicon, 0.1-3.0% manganese, 13-25% chromium, 13-40% nickel, 0.5-3.0% at least one kind selected from the group consisting of molybdenum and tungsten, 0.05-0.5% at least one kind selected from the group consisting of titanium, niobium and vanadium, and the balance iron and inevitable impurities. Boron of 0.001-0.01% may be further added to the alloy to improve creep strength while keeping improved high temperature corrosion resistance.

    摘要翻译: 一种具有改善的高温强度,改善的耐高温腐蚀性以及在其使用期间脆化的电阻率的锅炉管,包括外表面层和内部部分,所述外表面层基本上由0.03-0.20%碳组成 ,1.5-4.0%硅,0.1-3.0%锰,13-25%铬,13-40%镍,0.5-3.0%选自钼和钨的至少一种,0.05-0.5%的至少一种 选自钛,铌和钒组成的组,余量为铁和不可避免的杂质,其内部基本上由0.03-0.20%的碳,0.3-1.0%的硅,0.1-3.0的锰,13 -25%铬,13-40%镍,0.5-3.0%选自钼和钨的至少一种,0.05-0.5%选自钛,铌和钒中的至少一种,以及 余铁和不可避免的杂质。 可以进一步向合金中添加0.001-0.01%的硼以提高蠕变强度,同时保持改善的耐高温腐蚀性。