摘要:
A method for densification of the surface layer of an optionally sintered powder metal component comprising the steps of decarburizing the surface layer for softening the surface layer of the component, and densifying the surface layer of the component.
摘要:
A water atomized prealloyed chromium-free, iron-based steel powder is provided which comprises by weight-%: 0.05-0.4 V, 0.09-0.3 Mn, less than 0.1 Cr, less than 0.1 Mo, less than 0.1 Ni, less than 0.2 Cu, less than 0.1 C, less than 0.25 O, and less than 0.5 of unavoidable impurities, with the balance being iron.
摘要:
A water atomised prealloyed chromium-free, iron-based steel powder is provided which comprises by weight-%: 0.05-0.4 V, 0.09-0.3 Mn, less than 0.1 Cr, less than 0.1 Mo, less than 0.1 Ni, less than 0.2 Cu, less than 0.1 C, less than 0.25 O, and less than 0.5 of unavoidable impurities, with the balance being iron.
摘要:
A composition comprising water atomised prealloyed iron-based steel powder is provided which steel powder comprises by weight-%: 0.2-1.5 Cr, 0.05-0.4 V, 0.09-0.6 Mn, less than 0.1 Mo, less than 0.1 Ni, less than 0.2 Cu, less than 0.1 C, less than 0.25 O, less than 0.5 of unavoidable impurities, the balance being iron. A method of forming a sintered component, and component additionally are provided.
摘要:
A water atomised prealloyed iron-based steel powder is provided which comprises by weight-%: 0.4-2.0 Cr, 0.1-0.8 Mn, less than 0.1 V, less than 0.1 Mo, less than 0.1 Ni, less than 0.2 Cu, less than 0.1 C, less than 0.25 O, less than 0.5 of unavoidable impurities, and the balance being iron.
摘要:
A water atomised prealloyed iron-based steel powder is provided which comprises by weight-%: 0.2-1.5 Cr, 0.05-0.4 V, 0.09-0.6 Mn, less than 0.1 Mo, less than 0.1 Ni, less than 0.2 Cu, less than 0.1 C, less than 0.25 O, less than 0.5 of unavoidable impurities, the balance being iron.
摘要:
The present invention concerns a method for producing powder metal parts having a densified surface. The method comprises the steps: compacting an iron or iron-based powder by high velocity compacting technique to a density above 7.2 g/cm3 sintering the parts subjecting the parts to a surface densifying process.
摘要翻译:本发明涉及一种具有致密表面的粉末金属部件的制造方法。 该方法包括以下步骤:通过高速压实技术将铁或铁基粉末压实至7.2g / cm 3以上的密度烧结部件经受表面致密化处理的部件。