-
公开(公告)号:US20160068435A1
公开(公告)日:2016-03-10
申请号:US14785968
申请日:2014-04-24
发明人: Evan R. DANIELS , Per Just ANDERSON
CPC分类号: C04B18/027 , C04B14/16 , C04B28/02 , C04B41/4543 , C04B2111/00129 , C04B2111/28 , C04B2111/40 , C04B2201/32 , Y02W30/92 , Y02W30/94 , Y02W30/97 , C04B14/06 , C04B14/12 , C04B14/185 , C04B14/24 , C04B14/42 , C04B16/0633 , C04B16/0641 , C04B16/065 , C04B18/08 , C04B18/146 , C04B18/24 , C04B2103/0079 , C04B2103/20 , C04B14/28 , C04B18/141 , C04B22/143 , C04B24/06 , C04B24/14 , C04B24/38 , C04B24/383
摘要: An extrudable cement-based material is formed from a mixture that includes cement in the range of about 40 to 90% by wet weight percent, a lightweight expanded aggregate in the range of about 10 to 60% by wet weight percent, a secondary material in the range of about 0.1 to 50% by wet weight percent, a reinforcement fiber in the range of about 1 to 20% by wet weight percent, a rheology modifying agent in the range of about 0.5 to 10% by wet weight percent, a retarder in the range of about 0.1 to 8% by wet weight percent, and water in the range of 10 to 60% of a total wet material weight.
摘要翻译: 可挤出的基于水泥的材料由混合物形成,所述混合物包括以湿重百分比计约40-90%范围的水泥,轻质膨胀骨料的湿重百分比约为10-60% 约0.1〜50%的湿重百分比的范围,通过湿重百分数约1〜20%范围内的增强纤维,湿重百分比在约0.5〜10%的范围内的流变改性剂,缓凝剂 在约0.1至8%的湿重百分数的范围内,水的总湿重物料的10至60%。