Preparation method of perfluorinated polymer hollow fiber membrane
    1.
    发明授权
    Preparation method of perfluorinated polymer hollow fiber membrane 有权
    全氟聚合物中空纤维膜的制备方法

    公开(公告)号:US09211503B2

    公开(公告)日:2015-12-15

    申请号:US14358597

    申请日:2013-01-24

    Abstract: A preparation method of a perfluorinated polymer hollow fiber membrane comprises: evenly mixing a first mixture that is mixed by a perfluorinated polymer, PS, a polymer additive, and a composite pore-forming agent; evenly mixing a second mixture that is mixed by the first mixture and an organic liquid; under 300° C.-350° C., processing the second mixture with a melt to spin by a twin-screw extruder; extruding a hollow fiber by a hollow fiber spinneret; dipping the hollow fiber membrane into deionized water for 48 hours; putting the hollow fiber membrane aired into a concentrated sulfuric acid to process with a sulfonation; washing the hollow fiber membrane by deionized water; and drying the hollow fiber membrane; in such a manner that the hydrophilic perfluorinated polymer hollow fiber membrane is obtained.

    Abstract translation: 全氟化聚合物中空纤维膜的制备方法包括:将由全氟化聚合物PS,聚合物添加剂和复合成孔剂混合的第一混合物均匀混合; 均匀混合由第一混合物和有机液体混合的第二混合物; 在300℃-350℃下,用熔融物处理第二混合物通过双螺杆挤出机旋转; 通过中空纤维喷丝头挤出中空纤维; 将中空纤维膜浸入去离子水中48小时; 将中空纤维膜放入浓硫酸中进行磺化处理; 用去离子水清洗中空纤维膜; 并干燥中空纤维膜; 以这样的方式获得亲水性全氟化聚合物中空纤维膜。

    Preparation method of perfluorinated polymer hollow fiber membrane
    2.
    发明申请
    Preparation method of perfluorinated polymer hollow fiber membrane 审中-公开
    全氟聚合物中空纤维膜的制备方法

    公开(公告)号:US20140311968A1

    公开(公告)日:2014-10-23

    申请号:US14358597

    申请日:2013-01-24

    Abstract: A preparation method of a perfluorinated polymer hollow fiber membrane comprises: evenly mixing a first mixture that is mixed by a perfluorinated polymer, PS, a polymer additive, and a composite pore-forming agent; evenly mixing a second mixture that is mixed by the first mixture and an organic liquid; under 300° C.-350° C., processing the second mixture with a melt to spin by a twin-screw extruder; extruding a hollow fiber by a hollow fiber spinneret; dipping the hollow fiber membrane into deionized water for 48 hours; putting the hollow fiber membrane aired into a concentrated sulfuric acid to process with a sulfonation; washing the hollow fiber membrane by deionized water; and drying the hollow fiber membrane; in such a manner that the hydrophilic perfluorinated polymer hollow fiber membrane is obtained.

    Abstract translation: 全氟化聚合物中空纤维膜的制备方法包括:将由全氟化聚合物PS,聚合物添加剂和复合成孔剂混合的第一混合物均匀混合; 均匀混合由第一混合物和有机液体混合的第二混合物; 在300℃-350℃下,用熔融物处理第二混合物通过双螺杆挤出机旋转; 通过中空纤维喷丝头挤出中空纤维; 将中空纤维膜浸入去离子水中48小时; 将中空纤维膜放入浓硫酸中进行磺化处理; 用去离子水清洗中空纤维膜; 并干燥中空纤维膜; 以这样的方式获得亲水性全氟化聚合物中空纤维膜。