SULFIDE SOLID ELECTROLYTE MATERIAL, BATTERY, AND PRODUCING METHOD FOR SULFIDE SOLID ELECTROLYTE MATERIAL
    1.
    发明申请
    SULFIDE SOLID ELECTROLYTE MATERIAL, BATTERY, AND PRODUCING METHOD FOR SULFIDE SOLID ELECTROLYTE MATERIAL 有权
    硫化固体电解质材料,电池和硫化固体电解质材料的生产方法

    公开(公告)号:US20160064771A1

    公开(公告)日:2016-03-03

    申请号:US14783604

    申请日:2014-04-16

    Abstract: A sulfide solid electrolyte material with favorable ion conductivity and high reduction resistance. The object is attained by providing sulfide solid electrolyte material comprising: Li element; Ge element; P element; and S element, wherein the sulfide solid electrolyte material peaks at a position of 2θ=29.58°±0.50° in X-ray diffraction measurement using CuKα ray, the sulfide solid electrolyte material does not peak at a position of 2θ=27.33°±0.50° in X-ray diffraction measurement using CuKα ray or when diffraction intensity at the peak of 2θ=29.58°±0.50° is regarded as IA and diffraction intensity at the peak of 2θ=27.33°±0.50° is regarded as IB, a value of IB/IA is less than 1.0, and part of the P element in a crystal phase peaking at the position of 2θ=29.58°±0.50° is substituted with a B element.

    Abstract translation: 具有良好的离子传导性和高抗还原性的硫化物固体电解质材料。 本发明的目的是提供硫化物固体电解质材料,其包括:Li元素; Ge元素 P元素 和S元素,其中硫化物固体电解质材料在使用CuKα射线的X射线衍射测量中在2θ= 29.58°±0.50°的位置处峰值,硫化物固体电解质材料在2θ= 27.33°的位置处不峰值 使用CuKα射线的X射线衍射测定中的±0.50°,或者峰值为2θ时的衍射强度= 29.58°±0.50°的IA为1.0,峰值为2θ时的衍射强度= 27.33°±0.50°为 如图1B所示,IB / IA的值小于1.0,并且在2& t = 29.58°±0.50°的位置峰值的晶体相中的P元素的一部分被B元素取代。

    SULFIDE SOLID ELECTROLYTE MATERIAL, BATTERY, AND METHOD FOR PRODUCING SULFIDE SOLID ELECTROLYTE MATERIAL
    2.
    发明申请
    SULFIDE SOLID ELECTROLYTE MATERIAL, BATTERY, AND METHOD FOR PRODUCING SULFIDE SOLID ELECTROLYTE MATERIAL 审中-公开
    硫化固体电解质材料,电池及其制造方法

    公开(公告)号:US20150372345A1

    公开(公告)日:2015-12-24

    申请号:US14758712

    申请日:2013-12-18

    Abstract: Sulfide solid electrolyte material with favorable ion conductivity, wherein charge and discharge efficiency is inhibited from decreasing. Solves problem by providing a sulfide solid electrolyte material including a Li element, Si element, P element, S element and O element, having peak at position of 2θ=29.58°±0.50° in X-ray diffraction measurement using CuKα ray, wherein sulfide solid electrolyte material does not have peak at position of 2θ=27.33°±0.50° in X-ray diffraction measurement using CuKα ray, or in case of having peak at position of 2θ=27.33°±0.50°, value of IB/IA is 1 or less when diffraction intensity at peak of 2θ=29.58°±0.50° is regarded as IA and diffraction intensity at peak of 2θ=27.33°±0.50° is regarded as IB; and wherein molar fraction of O element to total of S element and O element is larger than 0.2.

    Abstract translation: 具有良好的离子传导性的硫化物固体电解质材料,其中抑制充放电效率的降低。 通过在使用CuKα射线的X射线衍射测定中提供包含Li元素,Si元素,P元素,S元素和O元素的硫化物固体电解质材料,其在2θ的位置具有峰值= 29.58°±0.50°,其中 硫化物固体电解质材料在使用CuKα射线的X射线衍射测定中,在2&位置的位置不具有峰值; = 27.33°±0.50°,或者在位置为2的情况下= 27.33°±0.50°,IB值 当IA的峰值处的衍射强度= 29.58°±0.50°时,IA值为1以下,2峰值时的衍射强度= 27.33°±0.50°为IB; 并且其中O元素与S元素和O元素总量的摩尔分数大于0.2。