公开(公告)号:US20230127585A1
公开(公告)日:2023-04-27
申请号:US18086612
申请日:2022-12-21
Applicant: Taiwan Textile Research Institute
Inventor: Shang-Chih Chou , Shao-Yen Chang , Chun-Hung Lin , Yuan-Pei Liao , Yi-Cang Lai
Abstract: A method of preparing a thermoplastic composition is provided. The method includes the following steps. A polyetherimide or a polyphenylene sulfide is provided. A polyimide is provided, wherein the glass transition temperature of the polyimide is between 128° C. and 169° C., the 10% thermogravimetric loss temperature of the polyimide is between 490° C. and 534° C., and when the polyimide is dissolved in N-methyl-2-pyrrolidone and the solid content of the polyimide is 30 wt %, the viscosity of the polyimide is between 100 cP and 250 cP. A melt process is performed to mix the polyetherimide and the polyimide or mix the polyphenylene sulfide and the polyimide to form a thermoplastic composition. Further, a thermoplastic composition is also provided.
-
公开(公告)号:US20210102321A1
公开(公告)日:2021-04-08
申请号:US16782082
申请日:2020-02-05
Applicant: Taiwan Textile Research Institute
Inventor: Shang-Chih Chou , Shao-Yen Chang , Chun-Hung Lin , Yuan-Pei Liao , Yi-Cang Lai
IPC: D04H1/56 , D04H3/16 , D04H1/4326 , D01F6/66 , D01F6/74
Abstract: A meltblown nonwoven fabric is provided. The meltblown nonwoven fabric includes a plurality of meltblown fibers adhered to each other. The material of each of the meltblown fibers includes a polyetherimide and a polyimide, or the material of each of the meltblown fibers includes a polyphenylene sulfide and a polyimide, wherein the glass transition temperature of the polyimide is between 128° C. and 169° C., the 10% thermogravimetric loss temperature of the polyimide is between 490° C. and 534° C., and when the polyimide is dissolved in N-methyl-2-pyrrolidone and the solid content of the polyimide is 30 wt %, the viscosity of the polyimide is between 100 cP and 250 cP.
-
公开(公告)号:US20210017382A1
公开(公告)日:2021-01-21
申请号:US16568267
申请日:2019-09-12
Applicant: Taiwan Textile Research Institute
Inventor: Shang-Chih Chou , Shao-Yen Chang , Chun-Hung Lin , Yuan-Pei Liao , Yi-Cang Lai
Abstract: A method of preparing a thermoplastic composition is provided. The method includes the following steps. A polyetherimide or a polyphenylene sulfide is provided. A polyimide is provided, wherein the glass transition temperature of the polyimide is between 128° C. and 169° C., the 10% thermogravimetric loss temperature of the polyimide is between 490° C. and 534° C., and when the polyimide is dissolved in N-methyl-2-pyrrolidone and the solid content of the polyimide is 30 wt %, the viscosity of the polyimide is between 100 cP and 250 cP. A melt process is performed to mix the polyetherimide and the polyimide or mix the polyphenylene sulfide and the polyimide to form a thermoplastic composition. Further, a thermoplastic composition is also provided.
-
公开(公告)号:US11572639B2
公开(公告)日:2023-02-07
申请号:US17035765
申请日:2020-09-29
Applicant: Taiwan Textile Research Institute
Inventor: Shang-Chih Chou , Shao-Yen Chang , Chun-Hung Lin , Yuan-Pei Liao , Yi-Cang Lai
Abstract: A fiber masterbatch including a polyetherimide, a polyethylene terephthalate, and a polyimide is provided. A glass transition temperature of the polyimide is between 140° C. and 170° C., a 10% thermogravimetric loss temperature of the polyimide is between 500° C. and 550° C., and when the polyimide is dissolved in N-methyl-2-pyrrolidone and a solid content of the polyimide is 15 wt %, a viscosity of the polyimide is between 80 cP and 230 cP. A melt spun fiber obtained by using the fiber masterbatch is also provided.
-
公开(公告)号:US20210301426A1
公开(公告)日:2021-09-30
申请号:US17035765
申请日:2020-09-29
Applicant: Taiwan Textile Research Institute
Inventor: Shang-Chih Chou , Shao-Yen Chang , Chun-Hung Lin , Yuan-Pei Liao , Yi-Cang Lai
Abstract: A fiber masterbatch including a polyetherimide, a polyethylene terephthalate, and a polyimide is provided. A glass transition temperature of the polyimide is between 140° C. and 170° C., a 10% thermogravimetric loss temperature of the polyimide is between 500° C. and 550° C., and when the polyimide is dissolved in N-methyl-2-pyrrolidone and a solid content of the polyimide is 15 wt %, a viscosity of the polyimide is between 80 cP and 230 cP. A melt spun fiber obtained by using the fiber masterbatch is also provided.
-
-
-
-