Titanium alloy, member made of the titanium alloy and method for
producing the titanium alloy member
    2.
    发明授权
    Titanium alloy, member made of the titanium alloy and method for producing the titanium alloy member 失效
    钛合金,由钛合金制成的部件和钛合金部件的制造方法

    公开(公告)号:US6007923A

    公开(公告)日:1999-12-28

    申请号:US659720

    申请日:1996-06-06

    IPC分类号: B23K35/00 B23K35/32 C22C14/00

    摘要: A joined tubular body comprises a titanium alloy pipe of which crystal grain is hard to coarsen at the time of welding or hot-extruding, which consists by weight percentage of at least one element selected from 0.01.about.10% of S, 0.01.about.10% of Se and 0.01.about.10% of Te (the total sum does not exceed 10%), one or both of 0.01.about.10% REM and 0.01.about.10% of Ca (the total sum does not exceed 10%), and the above pipe is joined to a titanium alloy pipe consisting of the above elements and also at least one element selected from Al.ltoreq.10%, V.ltoreq.25%, Sn.ltoreq.15%, Co.ltoreq.10%, Cu.ltoreq.10%, Ta.ltoreq.15%, Mn.ltoreq.10%, Hf.ltoreq.10%, W.ltoreq.10%, Si.ltoreq.0.5%, Nb.ltoreq.20%, Zr.ltoreq.10%, Mo.ltoreq.15%, and 0.ltoreq.0.1% (the total sum does not exceed 30%).

    摘要翻译: 连接的管体包括在焊接或热挤压时晶粒难以粗化的钛合金管,该重量百分比由选自0.01%S,0.01%,10%,10% 的Se和0.01差异Te的10%(总和不超过10%),0.01差异10%REM和0.01差异中的一种或两种,10%的Ca(总和不超过10%),以上 管连接到由上述元素组成的钛合金管中,并且还选自Al 10%,V 25%,Sn 15%,Co 10%,Cu 15%,Ta <15%,Mn <10%,Hf = 10%,W = 10%,Si≤0.5%,Nb≤20% / = 10%,Mo <15%,0 <= 0.1%(总和不超过30%)。