摘要:
A method for producing an optical film is provided and includes: simultaneously coating at least two coating solutions over a transparent support, the at least two coating solutions each containing a solvent and a solute; and drying the solvent in each of the at least two coating solutions to provide at least two coating layers. When the at least two coating layers are 1, 2, . . . n−1 and n layers in sequence from the outermost surface of the at least two coating layers toward the transparent support, n being an integer of 2 or more, the main component of the solute in the n-th layer is insoluble or sparingly soluble in the main component of the solvent in the (n−1)-th layer.
摘要:
An optical film, which comprises: a transparent support; and an optical layer on or above the transparent support, wherein the optical layer contains a thickening agent which shows a viscosity of 10 mPa·sec or more when added to 2-butanone in a content of 3% by mass, and the optical layer has a thickness of 5 μm or more.
摘要:
An antiglare film is provided, the antiglare film including: a support; and an antiglare layer including a surface that has asperities, wherein the antiglare layer contains at least first light-transmitting particles and second light-transmitting particles, the first light-transmitting particles have an average particle size that is 0.01 to 2.5 μm greater than an average thickness of the antiglare layer, the second light-transmitting particles have an average particle size that is at least 0.1 μm smaller than the average thickness of the antiglare layer, the first light-transmitting particles are contained in an amount of 0.1 to 2 mass % based on a total solid content in the antiglare layer, the second light-transmitting particles are contained in an amount of 2 to 30 mass % based on the total solid content in the antiglare layer, and the second light-transmitting particles include organic polymer-containing particles each of which has a core particle/shell layer structure.
摘要:
An antiglare film includes a transparent support; and an antiglare layer containing a binder and a fine particle, wherein the antiglare layer has an average thickness smaller than an average particle diameter of the fine particle, and the antiglare layer has a surface roughness skewness (Rsk) of from 0.5 to 1.5.
摘要:
A method for producing an optical film is provided and includes: simultaneously coating at least two coating solutions over a transparent support, the at least two coating solutions each containing a solvent and a solute; and drying the solvent in each of the at least two coating solutions to provide at least two coating layers. When the at least two coating layers are 1, 2, . . . n−1 and n layers in sequence from the outermost surface of the at least two coating layers toward the transparent support, n being an integer of 2 or more, the main component of the solute in the n-th layer is insoluble or sparingly soluble in the main component of the solvent in the (n−1)-th layer.
摘要:
An antireflection film includes, in a following order, a transparent substrate film; a medium refractive index layer; a high refractive index layer; and a low refractive index layer, wherein the medium refractive index layer is (A) a medium refractive index layer having a refractive index of 1.60 to 1.64 at a wavelength of 550 nm and a thickness of 55.0 to 65.0 nm, the high refractive index layer is (B) a high refractive index layer having a refractive index of 1.70 to 1.74 at a wavelength of 550 nm and a thickness of 105.0 to 115.0 nm, and the low refractive index layer is (C) a low refractive index layer having a refractive index of 1.32 to 1.37 at a wavelength of 550 nm and a thickness of 85.0 to 95.0 nm.
摘要:
An oil-in-water type emulsion coating composition having an aqueous phase and an oil phase, the oil-in-water type emulsion coating composition containing: an active energy ray-curable polyfunctional (meth)acrylate having three or more (meth)acryloyl groups within a molecule; and an organic solvent, in the oil phase, the organic solvent having a solubility of 30 g or less in 100 g of water and having a property capable of swelling or dissolving a substrate.
摘要:
An optical film, is provided, the optical film including: a support; and at least one antiglare layer having a surface that has asperities, wherein the at least one antiglare layer contains at least one kind of light transmitting particles including first light transmitting particles in an amount of 0.01 to 1 mass % based on a total solid content in the antiglare layer, the first light transmitting particles have an average particle size that is 0.1 to 4.0 μm greater than an average thickness of the antiglare layer, and a region θ(0.5) in which slope angles θ of the asperities of the surface of the antiglare layer lie within a range of 0°
摘要:
An oil-in-water type emulsion coating composition having an aqueous phase and an oil phase, the oil-in-water type emulsion coating composition containing: an active energy ray-curable polyfunctional (meth)acrylate having three or more (meth)acryloyl groups within a molecule; and an organic solvent, in the oil phase, the organic solvent having a solubility of 30 g or less in 100 g of water and having a property capable of swelling or dissolving a substrate.
摘要:
An optical film, is provided, the optical film including: a support; and at least one antiglare layer having a surface that has asperities, wherein the at least one antiglare layer contains at least one kind of light transmitting particles including first light transmitting particles in an amount of 0.01 to 1 mass % based on a total solid content in the antiglare layer, the first light transmitting particles have an average particle size that is 0.1 to 4.0 μm greater than an average thickness of the antiglare layer, and a region θ(0.5) in which slope angles θ of the asperities of the surface of the antiglare layer lie within a range of 0°