Welding contact tips for pulse applications
    1.
    发明授权
    Welding contact tips for pulse applications 有权
    用于脉冲应用的焊接触点

    公开(公告)号:US08383987B2

    公开(公告)日:2013-02-26

    申请号:US12776608

    申请日:2010-05-10

    申请人: Tiejun Ma

    发明人: Tiejun Ma

    IPC分类号: B23K9/28

    CPC分类号: B23K9/123

    摘要: A contact tip for a welding torch includes a body having a front discharge end, an opposite rear feed end, and a bore extending through the body. A cap is mounted on the body at the front end. The cap has an aperture generally aligned with the bore. The cap is composed of a material having an electrical conductivity between 1.74×107 and 4.35×107 Siemens per meter at 20° C. The body is composed of a material selected from the group consisting of copper and a copper alloy. The body has an electrical conductivity that is higher than the electrical conductivity of the cap. A portion of the bore at the front end of the body and at least a portion of the aperture in the cap define a contact area for a consumable electrode wire.

    摘要翻译: 用于焊炬的接触尖端包括具有前排出端,相对的后馈送端和延伸穿过本体的孔的主体。 在前端安装一个帽体。 盖具有通常与孔对准的孔。 该盖由在20℃下每米电导率为1.74×107-4.4×107西门子的材料构成。主体由选自铜和铜合金的材料组成。 主体的电导率高于盖的电导率。 在主体的前端处的孔的一部分和帽中的孔的至少一部分限定了可消耗电极线的接触面积。

    BAST FIBERS FOR PLASTICS REINFORCEMENT AND PREPARATION METHOD THEREOF
    2.
    发明申请
    BAST FIBERS FOR PLASTICS REINFORCEMENT AND PREPARATION METHOD THEREOF 审中-公开
    用于塑料加固的弹性纤维及其制备方法

    公开(公告)号:US20120070663A1

    公开(公告)日:2012-03-22

    申请号:US13321658

    申请日:2010-05-12

    IPC分类号: D02G3/00 D01D5/38

    摘要: The present invention refers to bast fibers for plastics reinforcement and preparation method thereof. The bast fibers are composed of the following components by weight ratio; 100 pts.wt. chopped bast fibers, 0.1˜100 pts.wt. bast fiber treating agent, 1˜10 pts.wt. Functional Polyolefin wax, 0.1˜10 pts.wt. coupling agent and 0.1˜0.5 pts.wt. antioxidant. The method includes the steps of: firstly, cut chopped bast fibers and soak them in sodium hydroxide solution, agitate the mixture, after rinse and drying of water, soak the fibers in the aqueous solution of bast fiber treating agent, then dry them and obtain surface-treated chopped bast fibers; secondly, add in order the chopped fibers, the coupling agent, the Functional Polyolefin wax and the antioxidant to a preheated kneader, agitate the mixture and thus obtain bast fibers for plastics reinforcement. Chopped bast fibers according to the invention present good color, rigidity and heat resistance, as well as excellent compatibility with plastics, and can be used in the preparation of high-performance short-bast-fiber\plastic composites, as reinforcement in the plastic matrix.

    摘要翻译: 本发明涉及用于塑料增强的韧皮纤维及其制备方法。 韧皮纤维按重量比由以下组分组成: 100 pts.wt 切碎的韧皮纤维,0.1〜100重量份 韧皮纤维处理剂,1〜10重量份 功能性聚烯烃蜡,0.1〜10重量份 偶联剂和0.1〜0.5重量份 抗氧化剂。 该方法包括以下步骤:首先将切碎的韧皮纤维浸泡在氢氧化钠溶液中,搅拌混合物,冲洗干燥后,将纤维浸泡在韧皮纤维处理剂水溶液中,然后干燥,得到 表面处理的切碎的韧皮纤维; 其次,将短切纤维,偶联剂,功能性聚烯烃蜡和抗氧化剂加入到预热的捏合机中,搅拌混合物,从而获得用于塑料增强的韧皮纤维。 根据本发明的切割韧皮纤维具有良好的颜色,刚性和耐热性,以及与塑料的良好相容性,并且可用于制备高性能短韧纤维\塑料复合材料,作为塑料基质中的增强 。

    WELDING SYSTEM AND METHOD HAVING CONTROLLED LINER CONTOUR AND WELDING WIRE CURVATURE
    3.
    发明申请
    WELDING SYSTEM AND METHOD HAVING CONTROLLED LINER CONTOUR AND WELDING WIRE CURVATURE 有权
    焊接系统和方法具有控制的衬里轮廓和焊接电线

    公开(公告)号:US20080314876A1

    公开(公告)日:2008-12-25

    申请号:US12128570

    申请日:2008-05-28

    IPC分类号: B23K9/28 B23K35/38

    CPC分类号: B23K9/122 B23K9/173

    摘要: A welding system, in certain embodiments, includes a torch having a neck with an arcuate portion, and a resilient jump liner disposed in the neck and extending through the arcuate portion. The resilient jump liner includes a pathway having a curvature configured to bend a welding wire passing through the pathway. The system also includes an annular support disposed about the resilient jump liner inside the neck, wherein the annular support is configured to at least substantially fix the curvature to force the welding wire to achieve a wire curvature. The system also includes a contact tip coupled to the neck, wherein the wire curvature is configured to bias the welding wire into substantially consistent contact with an interior pathway through the contact tip.

    摘要翻译: 在某些实施例中,焊接系统包括具有弓形部分的颈部的火炬和设置在颈部中并延伸穿过弧形部分的弹性跳跃衬套。 弹性跳线衬套包括具有弯曲被弯曲穿过通路的焊丝的曲率的路径。 该系统还包括围绕颈部内的弹性跳跃衬套设置的环形支撑件,其中环形支撑件构造成至少基本上固定曲率以迫使焊丝实现线弯曲。 该系统还包括联接到颈部的接触尖端,其中线曲率被配置为将焊丝偏置成与通过接触尖端的内部路径基本上一致的接触。

    Method for providing real-time monitoring of contact tip performance
    4.
    发明授权
    Method for providing real-time monitoring of contact tip performance 有权
    提供接触尖端性能实时监控的方法

    公开(公告)号:US08809738B2

    公开(公告)日:2014-08-19

    申请号:US13419506

    申请日:2012-03-14

    IPC分类号: B23K33/00 B23K9/12 B23K9/095

    CPC分类号: B23K9/123 B23K9/095

    摘要: A method for tracking contact tip deterioration in real time in accordance with the present invention includes establishing a reference that relates welding parameters during welding production to contact tip life; monitoring welding parameters of a contact tip during use; comparing the monitored welding parameters to the reference; providing real-time feedback to an operator; and predicting contact tip failure from the comparison.

    摘要翻译: 根据本发明的实时跟踪接触尖端劣化的方法包括建立在焊接生产期间将焊接参数与接触尖端寿命相关联的参考; 在使用过程中监测接触尖端的焊接参数; 将监测的焊接参数与参考值进行比较; 向操作员提供实时反馈; 并从比较中预测接触点故障。

    Method and apparatus to maintain welding current to compensate for deterioration of welding contact tip
    5.
    发明授权
    Method and apparatus to maintain welding current to compensate for deterioration of welding contact tip 有权
    保持焊接电流的方法和装置,以补偿焊接接触尖端的劣化

    公开(公告)号:US08710404B2

    公开(公告)日:2014-04-29

    申请号:US13419492

    申请日:2012-03-14

    IPC分类号: B23K9/10

    CPC分类号: B23K9/09

    摘要: A method of maintaining welding current to compensate for deterioration of a welding contact tip includes: monitoring in real time at least one of welding current and welding voltage during welding production; comparing the at least one of the welding current and the welding voltage to a reference value for a given set of parameters; and adjusting one or more welding parameters in real time to increase energy output in response to the comparison so that consistent energy is consumed across the welding arc, whereby the quality of the welding production is maintained as the welding contact tip is consumed.

    摘要翻译: 维持焊接电流以补偿焊接接触尖端的劣化的方法包括:在焊接生产期间实时监测焊接电流和焊接电压中的至少一个; 将所述焊接电流和焊接电压中的至少一个比较为给定参数集合的参考值; 并且实时调整一个或多个焊接参数以响应于比较来增加能量输出,从而在焊接电弧上消耗一致的能量,从而当焊接接触尖端被消耗时保持焊接生产的质量。

    Retaining head and contact tip for controlling wire contour and contacting point for GMAW torches
    6.
    发明授权
    Retaining head and contact tip for controlling wire contour and contacting point for GMAW torches 有权
    用于控制GMAW火炬的线轮廓和接触点的保持头和接触尖端

    公开(公告)号:US08450646B2

    公开(公告)日:2013-05-28

    申请号:US12125369

    申请日:2008-05-22

    IPC分类号: B23K9/173

    CPC分类号: B23K9/123 B23K9/295

    摘要: A retaining head for a MIG welding device includes a contact tip mounting end, an opposite retaining head mounting end, and a throughbore extending from one of the ends to the other end. A deflector is disposed along the throughbore and is adjustable for imparting a bend in welding wire passing through the throughbore. The deflector provides a straight wire contour for the welding wire that is fed out of the welding torch, while maintaining sufficient contact force between the welding wire and the contact tip. The deflector also reduces the effect of wire twist on the contact point between the welding wire and the contact tip.

    摘要翻译: 用于MIG焊接装置的保持头包括接触尖端安装端,相对的保持头安装端和从其中一个端部延伸到另一端的通孔。 导流板沿着通孔设置,并且可调节以在穿过通孔的焊丝中施加弯曲。 偏转器为从焊枪送出的焊丝提供直线轮廓,同时保持焊丝和接触尖端之间的足够的接触力。 偏转器还减少了线扭转对焊丝与接触尖端之间的接触点的影响。

    Front consumables for pulse GMAW torches
    7.
    发明授权
    Front consumables for pulse GMAW torches 有权
    用于脉冲GMAW手电筒的前置消耗品

    公开(公告)号:US08357877B2

    公开(公告)日:2013-01-22

    申请号:US12758347

    申请日:2010-04-12

    申请人: Tiejun Ma

    发明人: Tiejun Ma

    IPC分类号: H01L9/28

    摘要: A contact tip for a welding torch in accordance with the present invention includes an elongated, generally cylindrical body having a front contact end and an opposite rear retaining end. A central aperture is defined by an inner wall of the body. The aperture extends through the body from an opening at the rear retaining end to an opening at the front contact end. The aperture has a front portion and a wider diameter portion adjacent the front portion. The front portion generally has a length that is shorter than a length of the wider diameter portion. A consumable electrode wire fed through the aperture contacts the inner wall in the front portion but does not contact the inner wall in the wider diameter portion.

    摘要翻译: 根据本发明的用于焊炬的接触尖端包括具有前接触端和相对的后保持端的细长的大致圆柱形本体。 中心孔由身体的内壁限定。 孔从后保持端的开口延伸穿过主体到前接触端的开口。 该孔具有与前部相邻的前部和较宽的直径部。 前部通常具有比较宽直径部分的长度短的长度。 通过孔径供给的消耗电极线接触前部的内壁,但不与较宽直径部分的内壁接触。

    Method to monitor the life of the contact tip in robotic or automatic GMAW
    8.
    发明授权
    Method to monitor the life of the contact tip in robotic or automatic GMAW 有权
    监测机器人或自动GMAW中接触尖端寿命的方法

    公开(公告)号:US08354614B2

    公开(公告)日:2013-01-15

    申请号:US12836027

    申请日:2010-07-14

    IPC分类号: B23K9/095

    CPC分类号: B23K9/123 B23K9/295

    摘要: A method of monitoring contact tip useful life in a welding torch includes measuring at least one of welding current (I) and welding voltage (V) of the contact tip mounted in the welding torch. Deterioration of the contact tip is quantified based on one or both of (i) a decrease of the welding current and increase of a standard deviation of the welding current (sd_I), and (ii) an increase of the welding voltage. Deterioration of the contact tip may be quantified by calculating an index of contact tip life (ITL) based on the welding current and standard deviation of the welding current and/or by calculating a reference index of contact tip life (ITL_v) based on the welding voltage.

    摘要翻译: 一种监测焊枪的接触尖端使用寿命的方法包括测量安装在焊炬中的接触尖端的焊接电流(I)和焊接电压(V)中的至少一个。 基于(i)焊接电流的减小和焊接电流的标准偏差(sd_I)的增加中的一个或两个来定量接触尖端的劣化,以及(ii)焊接电压的增加。 可以通过基于焊接电流和焊接电流的标准偏差计算接触末端寿命指数(ITL)和/或通过基于焊接计算接触末端寿命的参考指数(ITL_v)来量化接触尖端的劣化 电压。

    METHOD FOR PROVIDING REAL-TIME MONITORING OF CONTACT TIP PERFORMANCE
    9.
    发明申请
    METHOD FOR PROVIDING REAL-TIME MONITORING OF CONTACT TIP PERFORMANCE 有权
    提供实时监控联系人提示性能的方法

    公开(公告)号:US20120234813A1

    公开(公告)日:2012-09-20

    申请号:US13419506

    申请日:2012-03-14

    IPC分类号: B23K33/00

    CPC分类号: B23K9/123 B23K9/095

    摘要: A method for tracking contact tip deterioration in real time in accordance with the present invention includes establishing a reference that relates welding parameters during welding production to contact tip life; monitoring welding parameters of a contact tip during use; comparing the monitored welding parameters to the reference; providing real-time feedback to an operator; and predicting contact tip failure from the comparison.

    摘要翻译: 根据本发明的实时跟踪接触尖端劣化的方法包括建立在焊接生产期间将焊接参数与接触尖端寿命相关联的参考; 在使用过程中监测接触尖端的焊接参数; 将监控的焊接参数与参考值进行比较; 向操作员提供实时反馈; 并从比较中预测接触点故障。

    METHOD TO MONITOR THE LIFE OF THE CONTACT TIP IN ROBOTIC OR AUTOMATIC GMAW
    10.
    发明申请
    METHOD TO MONITOR THE LIFE OF THE CONTACT TIP IN ROBOTIC OR AUTOMATIC GMAW 有权
    监测机器人或自动GMAW中接触提示生命的方法

    公开(公告)号:US20110073580A1

    公开(公告)日:2011-03-31

    申请号:US12836027

    申请日:2010-07-14

    IPC分类号: B23K9/095

    CPC分类号: B23K9/123 B23K9/295

    摘要: A method of monitoring contact tip useful life in a welding torch includes measuring at least one of welding current (I) and welding voltage (V) of the contact tip mounted in the welding torch. Deterioration of the contact tip is quantified based on one or both of (i) a decrease of the welding current and increase of a standard deviation of the welding current (sd_I), and (ii) an increase of the welding voltage. Deterioration of the contact tip may be quantified by calculating an index of contact tip life (ITL) based on the welding current and standard deviation of the welding current and/or by calculating a reference index of contact tip life (ITL_v) based on the welding voltage.

    摘要翻译: 一种监测焊枪的接触尖端使用寿命的方法包括测量安装在焊炬中的接触尖端的焊接电流(I)和焊接电压(V)中的至少一个。 基于(i)焊接电流的减小和焊接电流的标准偏差(sd_I)的增加中的一个或两个来定量接触尖端的劣化,以及(ii)焊接电压的增加。 可以通过基于焊接电流和焊接电流的标准偏差计算接触末端寿命指数(ITL)和/或通过基于焊接计算接触末端寿命的参考指数(ITL_v)来量化接触尖端的劣化 电压。