Roasting of mixed sulphide ores or concentrates
    3.
    发明授权
    Roasting of mixed sulphide ores or concentrates 失效
    混合硫化矿石或浓缩物的焙烧

    公开(公告)号:US4478794A

    公开(公告)日:1984-10-23

    申请号:US471709

    申请日:1983-03-03

    IPC分类号: C01G9/02 C22B1/02 C22B1/24

    CPC分类号: C01G9/02 C22B1/02 C22B1/2406

    摘要: In the roasting (oxidation) of mixed zinc sulphide/lead sulphide concentrates, to give an oxidic product for reduction, improved sulphur elimination and reduced lead volatilization are achieved by mixing 2-20% by weight of zinc oxide with the mixed sulphide materials, forming pellets of 2-15 mm diameter and roasting these under controlled oxidation conditions, firstly at a lower temperature and then at a higher temperature; preferably at 850.degree.-950.degree. C. for the first stage and at 950.degree.-1050.degree. C. for the last stage.