POLYARYLENE SULFIDE AND METHOD FOR PRODUCING SAME (AS AMENDED)

    公开(公告)号:US20170130005A1

    公开(公告)日:2017-05-11

    申请号:US15321952

    申请日:2015-06-30

    CPC classification number: C08G75/0259 C08G75/02 C08G75/0213 C08G75/0281

    Abstract: There is provided a polyarylene sulfide configured to satisfy (1) to (4): (1) having a weight-average molecular weight of not less than 10000; (2) having a polydispersity of not greater than 2.5, wherein the polydispersity is expressed by a ratio of the weight-average molecular weight to a number-average molecular weight; (3) having a weight reduction on heating that satisfies an expression of ΔWr=(W1−W2)/W1×100≦0.18(%) (where ΔWr denotes a weight reduction ratio (%) and is a value calculated from a sample weight (W2) at temperature reaching 330° C. relative to a sample weight (W1) at temperature reaching 100° C. in thermogravimetric analysis at a temperature rise rate of 20° C./minute in a non-oxidizing atmosphere at ordinary pressure); and (4) having a nitrogen content of not greater than 200 ppm.

    GARMENT
    4.
    发明申请
    GARMENT 有权

    公开(公告)号:US20220312862A1

    公开(公告)日:2022-10-06

    申请号:US17642261

    申请日:2020-08-05

    Abstract: To provide a garment capable of suppressing a stuffy feeling and a hot feeling in the garment regardless of the presence or absence of air blowing from a blower fan, maintaining a comfortable environment in the garment, and having excellent wearing comfort, the garment includes a fabric mainly formed of hygroscopic fibers as constituent fibers, the fabric having air permeability of 45 cm3/cm2/s or less; and at least one air inlet for taking outside air into the garment.

Patent Agency Ranking