1.
公开(公告)号:US06281278B1
公开(公告)日:2001-08-28
申请号:US09331883
申请日:1999-06-29
申请人: Toru Takase , Tatsuji Maekawa , Hideshi Kurihara , Takuo Nakao
发明人: Toru Takase , Tatsuji Maekawa , Hideshi Kurihara , Takuo Nakao
IPC分类号: C08K322
CPC分类号: B29B7/7461 , B29B7/007 , B29B7/325 , B29B7/40 , B29C47/362 , B29K2067/00 , C08J3/203 , C08J3/226
摘要: A process for preparing a modified thermoplastic resin composition by incorporating a modifier-containing thermoplastic resin into a transport line of a thermoplastic resin, comprising subjecting the resin to static mixing and to dynamic mixing by passing the resin through a dynamic mixing apparatus having a mixing blade unit and a power unit for driving the mixing blade unit and provided in the same transport line, as well as a modified thermoplastic resin composition prepared by the process and having a filtration pressure increase rate of no greater than 10 kg/cm2/hr when filtration is performed using a double layer of 2400 mesh wire filters with an inner diameter of 64 mm&phgr;, at a melting point of the modified thermoplastic resin or a temperature of from 20° C. to 100° C. higher than the plasticizing point of the resin and at a filtration rate of 33.3 g/min.
摘要翻译: 一种制备改性热塑性树脂组合物的方法,其通过将含改性剂的热塑性树脂掺入到热塑性树脂的输送线中,包括使树脂经静态混合和使树脂通过具有混合叶片的动态混合装置进行动态混合 单元和用于驱动混合叶片单元并设置在相同输送管线中的动力单元以及通过该方法制备的改性热塑性树脂组合物,并且当过滤时具有不大于10kg / cm 2 / hr的过滤压力增加率 使用内径为64mmφ的双层2400目的丝网过滤器,在改性热塑性树脂的熔点或比树脂的增塑点高20℃至100℃的温度下进行 并以33.3g / min的过滤速率。