    摘要: In a method of preparing a boron carbide material, boron carbide powder is washed with essentially pure water at an elevated temperature to generate washed boron carbide powder. The washed boron carbide powder is combined with a sintering aid. The mixture of the boron carbide powder and the sintering aid is pressed to form a shaped material, and the shaped material is sintered. A sintered boron carbide material comprises a boron carbide component that includes boron carbide, elemental carbon, and not more than about 0.6 wt % of oxygen on the basis of the total weight of the boron carbide component. The sintered boron carbide material has a density of at least about 99% of the theoretical density. Another sintered boron carbide material comprises a boron carbide component that includes boron carbide, silicon carbide, elemental carbon, and not more than about 0.3 wt % oxygen on the basis of the total weight of the boron carbide component, and has a density of at least about 97% of the theoretical density.

    摘要翻译: 在制备碳化硼材料的方法中,碳化硼粉末在高温下用基本上纯的水洗涤以产生洗涤的碳化硼粉末。 将洗涤的碳化硼粉末与烧结助剂组合。 将碳化硼粉末和烧结助剂的混合物压制以形成成形材料,并将成形材料烧结。 烧结碳化硼材料包括碳化硼组分,其包含碳化硼,元素碳,基于碳化硼组分的总重量不超过约0.6重量%的氧。 烧结碳化硼材料的密度至少为理论密度的约99%。 另一种烧结碳化硼材料包括碳化硼组分,其包含碳化硼,碳化硅,元素碳和基于碳化硼组分的总重量不大于约0.3重量%的氧,并且至少具有至少 约97%的理论密度。

    Method of preparing pressureless sintered, highly dense boron carbide materials
    2.
    发明授权
    Method of preparing pressureless sintered, highly dense boron carbide materials 失效
    制备无压烧结,高密度碳化硼材料的方法

    公开(公告)号:US07919040B2

    公开(公告)日:2011-04-05

    申请号:US12221916

    申请日:2008-08-07

    IPC分类号: B28B3/00

    摘要: In a method of preparing a boron carbide material, boron carbide powder is washed with essentially pure water at an elevated temperature to generate washed boron carbide powder. The washed boron carbide powder is combined with a sintering aid. The mixture of the boron carbide powder and the sintering aid is pressed to form a shaped material, and the shaped material is sintered. A sintered boron carbide material comprises a boron carbide component that includes boron carbide, elemental carbon, and not more than about 0.6 wt % of oxygen on the basis of the total weight of the boron carbide component. The sintered boron carbide material has a density of at least about 99% of the theoretical density. Another sintered boron carbide material comprises a boron carbide component that includes boron carbide, silicon carbide, elemental carbon, and not more than about 0.3 wt % oxygen on the basis of the total weight of the boron carbide component, and has a density of at least about 97% of the theoretical density.

    摘要翻译: 在制备碳化硼材料的方法中,碳化硼粉末在高温下用基本上纯的水洗涤以产生洗涤的碳化硼粉末。 将洗涤的碳化硼粉末与烧结助剂组合。 将碳化硼粉末和烧结助剂的混合物压制以形成成形材料,并将成形材料烧结。 烧结碳化硼材料包括碳化硼组分,其包含碳化硼,元素碳,基于碳化硼组分的总重量不超过约0.6重量%的氧。 烧结碳化硼材料的密度至少为理论密度的约99%。 另一种烧结碳化硼材料包括碳化硼组分,其包含碳化硼,碳化硅,元素碳和基于碳化硼组分的总重量不大于约0.3重量%的氧,并且至少具有至少 约97%的理论密度。

    METHOD OF PREPARING PRESSURELESS SINTERED, HIGHLY DENSE BORON CARBIDE MATERIALS
    3.
    发明申请
    METHOD OF PREPARING PRESSURELESS SINTERED, HIGHLY DENSE BORON CARBIDE MATERIALS 审中-公开
    制备无压烧结的方法,高密度硼硼碳材料

    公开(公告)号:US20110160035A1

    公开(公告)日:2011-06-30

    申请号:US13045356

    申请日:2011-03-10

    IPC分类号: C04B35/563 C04B35/565

    摘要: In a method of preparing a boron carbide material, boron carbide powder is washed with essentially pure water at an elevated temperature to generate washed boron carbide powder. The washed boron carbide powder is combined with a sintering aid. The mixture of the boron carbide powder and the sintering aid is pressed to form a shaped material, and the shaped material is sintered. A sintered boron carbide material comprises a boron carbide component that includes boron carbide, elemental carbon, and not more than about 0.6 wt % of oxygen on the basis of the total weight of the boron carbide component. The sintered boron carbide material has a density of at least about 99% of the theoretical density. Another sintered boron carbide material comprises a boron carbide component that includes boron carbide, silicon carbide, elemental carbon, and not more than about 0.3 wt % oxygen on the basis of the total weight of the boron carbide component, and has a density of at least about 97% of the theoretical density.

    摘要翻译: 在制备碳化硼材料的方法中,碳化硼粉末在高温下用基本上纯的水洗涤以产生洗涤的碳化硼粉末。 将洗涤的碳化硼粉末与烧结助剂组合。 将碳化硼粉末和烧结助剂的混合物压制以形成成形材料,并将成形材料烧结。 烧结碳化硼材料包括碳化硼组分,其包含碳化硼,元素碳,基于碳化硼组分的总重量不超过约0.6重量%的氧。 烧结碳化硼材料的密度至少为理论密度的约99%。 另一种烧结碳化硼材料包括碳化硼组分,其包含碳化硼,碳化硅,元素碳和基于碳化硼组分的总重量不大于约0.3重量%的氧,并且至少具有至少 约97%的理论密度。

    METHODS OF FORMING SINTERED BORON CARBIDE
    4.
    发明申请
    METHODS OF FORMING SINTERED BORON CARBIDE 审中-公开
    烧结碳硼化物的方法

    公开(公告)号:US20110227259A1

    公开(公告)日:2011-09-22

    申请号:US12841474

    申请日:2010-07-22

    IPC分类号: C04B35/645 C04B35/64

    摘要: A method of forming a sintered boron carbide body includes washing boron carbide powder with essentially pure water at an elevated temperature to generate low oxygen boron carbide powder, mixing a sintering aid and a pressing aid with the low oxygen boron carbide powder to form a green mixture, and shaping the green mixture into a green boron carbide body. The method can include mixing titanium carbide powder having an average particle diameter in a range of between about 5 nm and about 100 nm with the low oxygen boron carbide powder. The method can further include sintering the green boron carbide body, and hot isostatic pressing the sintered body, to a density greater than about 98.5% of the theoretical density (TD) of boron carbide. Alternatively, the method can include sintering the shaped boron carbide green body at a temperature greater than about 2,200° C., to thereby form a eutectic liquid solid solution of B4C/SiC, forming a sintered boron carbide body with a density greater than about 98% TD.