Nickel-base alloys and articles made therefrom
    1.
    发明授权
    Nickel-base alloys and articles made therefrom 有权
    镍基合金及其制品

    公开(公告)号:US07985304B2

    公开(公告)日:2011-07-26

    申请号:US11737361

    申请日:2007-04-19

    IPC分类号: C22C19/05

    CPC分类号: C22C19/056 C22C19/05

    摘要: A nickel-base alloy having favorable toughness and thermal fatigue resistance comprises, in weight percentages based on total alloy weight: 9 to 20 chromium; 25 to 35 iron; 1 to 3 molybdenum; 3.0 to 5.5 niobium; 0.2 to 2.0 aluminum; 0.3 to 3.0 titanium; less than 0.10 carbon; no more than 0.01 boron; nickel; and incidental impurities. Also disclosed are die casting dies, other tooling, and other articles of manufacture made from or comprising the nickel-base alloy.

    摘要翻译: 具有良好的韧性和耐热疲劳性的镍基合金包括以总合金重量为基准的重量百分数:9至20铬; 25至35铁 1〜3钼; 3.0〜5.5铌; 0.2〜2.0铝; 0.3〜3.0钛; 小于0.10碳; 不超过0.01硼; 镍; 和杂质。 还公开了由镍基合金制成或包括镍基合金的压铸模,其它模具和其它制品。

    Nickel-base alloys and articles made therefrom
    2.
    发明授权
    Nickel-base alloys and articles made therefrom 有权
    镍基合金及其制品

    公开(公告)号:US08394210B2

    公开(公告)日:2013-03-12

    申请号:US13101207

    申请日:2011-05-05

    IPC分类号: C22C19/05

    CPC分类号: C22C19/056 C22C19/05

    摘要: A nickel-base alloy having favorable toughness and thermal fatigue resistance comprises, in weight percentages based on total alloy weight: 9 to 12 chromium; 25 to 35 iron; 1 to 3 molybdenum; 3.0 to 5.5 niobium; 0.2 to 2.0 aluminum; 0.3 to 3.0 titanium; less than 0.10 carbon; no more than 0.01 boron; nickel; and incidental impurities. Also disclosed are die casting dies, other tooling, and other articles of manufacture made from or comprising the nickel-base alloy.

    摘要翻译: 具有良好韧性和耐热疲劳性的镍基合金包括以总合金重量为基准的重量百分比:9-12铬; 25至35铁; 1〜3钼; 3.0〜5.5铌; 0.2〜2.0铝; 0.3〜3.0钛; 小于0.10碳; 不超过0.01硼; 镍; 和杂质。 还公开了由镍基合金制成或包括镍基合金的压铸模,其它模具和其它制品。

    NICKEL-BASE ALLOYS AND ARTICLES MADE THEREFROM
    3.
    发明申请
    NICKEL-BASE ALLOYS AND ARTICLES MADE THEREFROM 有权
    镍基合金及其制品

    公开(公告)号:US20110206553A1

    公开(公告)日:2011-08-25

    申请号:US13101207

    申请日:2011-05-05

    IPC分类号: C22C19/05 C22C30/00

    CPC分类号: C22C19/056 C22C19/05

    摘要: A nickel-base alloy having favorable toughness and thermal fatigue resistance comprises, in weight percentages based on total alloy weight: 9 to 12 chromium; 25 to 35 iron; 1 to 3 molybdenum; 3.0 to 5.5 niobium; 0.2 to 2.0 aluminum; 0.3 to 3.0 titanium; less than 0.10 carbon; no more than 0.01 boron; nickel; and incidental impurities. Also disclosed are die casting dies, other tooling, and other articles of manufacture made from or comprising the nickel-base alloy.

    摘要翻译: 具有良好韧性和耐热疲劳性的镍基合金包括以总合金重量为基准的重量百分比:9-12铬; 25至35铁; 1〜3钼; 3.0〜5.5铌; 0.2〜2.0铝; 0.3〜3.0钛; 小于0.10碳; 不超过0.01硼; 镍; 和杂质。 还公开了由镍基合金制成或包括镍基合金的压铸模,其它模具和其它制品。

    NICKEL-BASE ALLOYS AND ARTICLES MADE THEREFROM
    4.
    发明申请
    NICKEL-BASE ALLOYS AND ARTICLES MADE THEREFROM 有权
    镍基合金及其制品

    公开(公告)号:US20080257457A1

    公开(公告)日:2008-10-23

    申请号:US11737361

    申请日:2007-04-19

    IPC分类号: C22C19/05

    CPC分类号: C22C19/056 C22C19/05

    摘要: A nickel-base alloy having favorable toughness and thermal fatigue resistance comprises, in weight percentages based on total alloy weight: 9 to 20 chromium; 25 to 35 iron; 1 to 3 molybdenum; 3.0 to 5.5 niobium; 0.2 to 2.0 aluminum; 0.3 to 3.0 titanium; less than 0.10 carbon; no more than 0.01 boron; nickel; and incidental impurities. Also disclosed are die casting dies, other tooling, and other articles of manufacture made from or comprising the nickel-base alloy.

    摘要翻译: 具有良好的韧性和耐热疲劳性的镍基合金包括以总合金重量为基准的重量百分数:9至20铬; 25至35铁 1〜3钼; 3.0〜5.5铌; 0.2〜2.0铝; 0.3〜3.0钛; 小于0.10碳; 不超过0.01硼; 镍; 和杂质。 还公开了由镍基合金制成或包括镍基合金的压铸模,其它模具和其它制品。

    Method of forming corrosion resistant coating
    5.
    发明授权
    Method of forming corrosion resistant coating 失效
    形成耐腐蚀涂层的方法

    公开(公告)号:US4529616A

    公开(公告)日:1985-07-16

    申请号:US575233

    申请日:1984-01-30

    申请人: John W. Smythe

    发明人: John W. Smythe

    IPC分类号: C22C19/05 C23C4/06 B05D1/08

    CPC分类号: C22C19/055 C23C4/067

    摘要: An improved thermal spray nickel base alloy powder which forms an extremely tenacious, dense corrosion resistant coating on metal parts subject to a corrosive environment. The disclosed thermal spray powder is a nickel base alloy having 20 to 40% by weight molybdenum, and 12 to 20% by weight chromium, and preferably includes 0 to 10% by weight iron and 0.03 to 2% by weight copper plus vanadium. The metal alloy powder is preferably formed by atomizing the molten alloy, and the coating is preferably formed by thermal or plasma spray.

    摘要翻译: 一种改进的热喷镍基合金粉末,可在有腐蚀性环境的金属部件上形成极其坚固,致密的耐腐蚀涂层。 所公开的热喷涂粉末是具有20〜40重量%的钼和12〜20重量%的铬的镍基合金,优选含有0〜10重量%的铁和0.03〜2重量%的铜加钒。 金属合金粉末优选通过使熔融合金雾化而形成,优选通过热等离子体喷涂形成涂层。

    Corrosion resistant thermal spray alloy and coating method
    6.
    发明授权
    Corrosion resistant thermal spray alloy and coating method 失效
    耐腐蚀热喷涂合金和涂层方法

    公开(公告)号:US4453976A

    公开(公告)日:1984-06-12

    申请号:US411197

    申请日:1982-08-25

    申请人: John W. Smythe

    发明人: John W. Smythe

    IPC分类号: C22C19/05 C23C4/06 B05D1/10

    CPC分类号: C22C19/055 C23C4/067

    摘要: An improved thermal spray nickel base alloy powder which forms an extremely tenacious, dense corrosion resistant coating on metal parts subject to a corrosive environment. The disclosed thermal spray powder is a nickel base alloy having 20 to 40% by weight molybdenum, and 12 to 20% by weight chromium, and preferably includes 0 to 10% by weight iron and 0.03 to 2% by weight copper plus vanadium. The metal alloy powder is preferably formed by atomizing the molten alloy, and the coating is preferably formed by thermal or plasma spray.

    摘要翻译: 一种改进的热喷镍基合金粉末,可在有腐蚀性环境的金属部件上形成极其坚固,致密的耐腐蚀涂层。 所公开的热喷涂粉末是具有20〜40重量%的钼和12〜20重量%的铬的镍基合金,优选含有0〜10重量%的铁和0.03〜2重量%的铜加钒。 金属合金粉末优选通过使熔融合金雾化而形成,优选通过热等离子体喷涂形成涂层。