    摘要: A composition or concentrate for preserving wood, which comprises 0.001-5% by weight of cyano-(4-fluoro-3-phenoxyphenyl)-methyl 3-(2,2-dichloroethenyl)-2,2-dimethylcyclopropanecarboxylate and/or (pentafluorophenyl)-methyl 1R, 3R-3-(2,2-dichloroethenyl)-2,2-dimethylcyclopropanecarboxylate or enantiomeric compounds thereof and more than 75% by weight, preferably more than 90% by weight, of a mixture comprising at least one binder at least one diluent, and optionally at least one emulsifier and/or wetting agent or mixture thereof. The binder in the wood preservative or concentrate (calculated as solids) amounts to at least 1% by weight, preferably at least 4% by weight of the composition. An alkyd resin and/or a vegetable drying oil is preferably used in the composition as the organic binder for preventing or reducing damage to beneficial insects.

    摘要翻译: 用于保存木材的组合物或浓缩物,其包含0.001-5重量%的氰基 - (4-氟-3-苯氧基苯基) - 3-(2,2-二氯乙烯基)-2,2-二甲基环丙烷甲酸甲酯和/或(五氟苯基 ) - 1R,3R-3-(2,2-二氯乙烯基)-2,2-二甲基环丙烷甲酸甲酯或其对映异构体化合物和大于75重量%,优选大于90重量%的包含至少一种粘合剂 至少一种稀释剂和任选的至少一种乳化剂和/或润湿剂或其混合物。 木材防腐剂或浓缩物中的粘合剂(按固体计算)为组合物重量的至少1重量%,优选至少4重量%。 组合物中优选使用醇酸树脂和/或植物性干性油作为有机粘合剂,以防止或减少对有害昆虫的损害。