公开(公告)号:US4411702A
公开(公告)日:1983-10-25
申请号:US357636
申请日:1982-03-12
CPC分类号: C04B28/08 , C04B20/1051
摘要: A method for sheet forming a remarkably waterproof gypsum hardened body, in which a main component consisting of gypsum dihydrate, slag and calcium hydroxide and additives are added with a part of the main component coated with a hydrophobic diorganopolysiloxane fluid having a kinetic viscosity of 10-10,000 CS at 25.degree. to be sheet formed and cured. The hydrophobic diorganopolysiloxane fluid is uniformly dispersed through the sheet formed gypsum hardened body and its strong water repelling property makes the gypsum hardened body remarkably waterproof to be used suitably as both interior and outdoor construction materials.
摘要翻译: 一种形成非常防水的石膏硬化体的方法,其中添加由二水合石膏,炉渣和氢氧化钙和添加剂组成的主要组分,其中主要组分的一部分涂覆有动态粘度为10的疏水性二有机聚硅氧烷流体, 25℃的10,000 CS成片并固化。 疏水性二有机聚硅氧烷流体通过片状石膏硬化体均匀分散,其强斥水性使石膏硬化体显着防水,适用于室内外建筑材料。
-
公开(公告)号:US4717503A
公开(公告)日:1988-01-05
申请号:US522671
申请日:1983-08-12
申请人: Yoshio Makino , Toshiaki Kakinuma , Tomio Iwata , Masumi Itoh , Takayoshi Hirose
发明人: Yoshio Makino , Toshiaki Kakinuma , Tomio Iwata , Masumi Itoh , Takayoshi Hirose
CPC分类号: E21C37/06 , C04B28/10 , C04B41/0009 , E04G23/08
摘要: A demolition agent for brittle materials in the form of a powder mixture comprising 100 parts by weight of quicklime, 0.05 to 5 parts by weight of a carbonate and either or both of 0.01 to 5 parts by weight of a hydroxy-carboxylic acid or its salt and 0.1 to 5 parts by weight of a fluidization agent. This demolition agent is used by admixing with water to obtain an aqueous slurry, pouring the slurry into a hole drilled in a brittle material and allowing it to stand to demolish the brittle material by means of expansive pressure from the slurry.
摘要翻译: 一种粉末混合物形式的脆性材料的破坏剂,包括100重量份的生石灰,0.05-5重量份的碳酸盐和0.01-5重量份的羟基羧酸或其盐 和0.1〜5重量份的流化剂。 这种拆除剂通过与水混合使用以获得含水浆料,将浆料倒入钻孔在脆性材料中的孔中,并通过来自浆料的膨胀压力使其静置以破坏脆性材料。
-