公开(公告)号:US09127372B2
公开(公告)日:2015-09-08
申请号:US11813805
申请日:2006-01-11
CPC分类号: C30B7/10 , B01J3/04 , C23C30/00 , C30B35/002 , Y10T29/49826 , Y10T117/10 , Y10T117/1096
摘要: An object of the present invention is to manufacture single crystals of high quality on an industrial production scale by preventing impurities from being mixed in single crystals when the single crystals are produced by the solvothermal method.A pressure vessel body 1, in which a supercritical state is maintained, is made of heat resistant alloy, a portion of the pressure vessel body is open, a corrosion-resistant mechanical lining 5 is provided on an inner face of the pressure vessel and on an entire outer circumferential edge of the opening, and the opening is sealed by an airtight mating face formed out of a corrosion-resistant mechanical lining, which is formed on the outer circumferential edge of the opening, and by an airtight mating face of the corrosion-resistant mechanical lining cover 6 on an inner face of the cover 3 through a corrosion-resistant gasket member. Since the pressure vessel body and the inner face of the cover are covered with the corrosion-resistant mechanical lining, corrosion can be prevented. The corrosion-resistant mechanical lining ensures the sealing property on the airtight mating face between the pressure vessel body and the cover and further effectively prevents corrosion in the airtight sealing portion and it becomes possible to repeatedly open and close the airtight sealing portion.
摘要翻译: 本发明的目的是通过在通过溶剂热法制造单晶时,通过防止杂质混合在单晶中,在工业生产规模上制造高质量的单晶。 保持超临界状态的压力容器主体1由耐热合金制成,压力容器主体的一部分打开,在压力容器的内表面上设置耐腐蚀的机械衬里5, 开口的整个外圆周边缘,并且开口由形成在开口的外周边缘上的耐腐蚀机械衬里形成的气密配合面和由腐蚀的气密配合面密封 通过耐腐蚀的垫圈构件在盖3的内表面上具有耐力的机械衬里盖6。 由于压力容器主体和盖的内表面被耐腐蚀的机械衬里覆盖,所以可以防止腐蚀。 耐腐蚀机械衬里确保了压力容器主体和盖之间的气密配合面上的密封性能,并且进一步有效地防止了气密密封部分中的腐蚀,并且可以重复地打开和关闭气密密封部分。
-
公开(公告)号:US20090013926A1
公开(公告)日:2009-01-15
申请号:US11813805
申请日:2006-01-11
IPC分类号: B01J3/04
CPC分类号: C30B7/10 , B01J3/04 , C23C30/00 , C30B35/002 , Y10T29/49826 , Y10T117/10 , Y10T117/1096
摘要: An object of the present invention is to manufacture single crystals of high quality on an industrial production scale by preventing impurities from being mixed in single crystals when the single crystals are produced by the solvothermal method.A pressure vessel body 1, in which a supercritical state is maintained, is made of heat resistant alloy, a portion of the pressure vessel body is open, a corrosion-resistant mechanical lining 5 is provided on an inner face of the pressure vessel and on an entire outer circumferential edge of the opening, and the opening is sealed by an airtight mating face formed out of a corrosion-resistant mechanical lining, which is formed on the outer circumferential edge of the opening, and by an airtight mating face of the corrosion-resistant mechanical lining cover 6 on an inner face of the cover 3 through a corrosion-resistant gasket member. Since the pressure vessel body and the inner face of the cover are covered with the corrosion-resistant mechanical lining, corrosion can be prevented. The corrosion-resistant mechanical lining ensures the sealing property on the airtight mating face between the pressure vessel body and the cover and further effectively prevents corrosion in the airtight sealing portion and it becomes possible to repeatedly open and close the airtight sealing portion.
摘要翻译: 本发明的目的是通过在通过溶剂热法制造单晶时,通过防止杂质混合在单晶中,在工业生产规模上制造高质量的单晶。 保持超临界状态的压力容器主体1由耐热合金制成,压力容器主体的一部分打开,在压力容器的内表面上设置耐腐蚀的机械衬里5, 开口的整个外圆周边缘,并且开口由形成在开口的外周边缘上的耐腐蚀机械衬里形成的气密配合面和由腐蚀的气密配合面密封 通过耐腐蚀的垫圈构件在盖3的内表面上具有耐力的机械衬里盖6。 由于压力容器主体和盖的内表面被耐腐蚀的机械衬里覆盖,所以可以防止腐蚀。 耐腐蚀机械衬里确保了压力容器主体和盖之间的气密配合面上的密封性能,并且进一步有效地防止了气密密封部分中的腐蚀,并且可以重复地打开和关闭气密密封部分。
-
公开(公告)号:US06402991B1
公开(公告)日:2002-06-11
申请号:US09425222
申请日:1999-10-22
IPC分类号: C04B3510
CPC分类号: C04B35/18
摘要: The function of a functional material is enhanced by kneading a metallic powder, a metallic compound, or a functional mineral powder with a far-IR-radiating ceramic composition into a shape suitable for the application. A shaped article of a function-enhanced ceramic is obtained by kneading a powder of a far-IR-radiating material comprising a ceramic composition containing 52.5-70 wt % SiO2 and 20-47 wt % Al2O3 in an amount of 30 wt % or more and a metallic powder, a metallic compound, or a functional mineral powder; shaping and drying the mixture; and firing.
摘要翻译: 通过将金属粉末,金属化合物或功能性矿物粉末与远红外辐射陶瓷组合物捏合成适合于该应用的形状来增强功能材料的功能。 功能增强陶瓷的成型制品通过将包含含有52.5-70重量%SiO 2和20-47重量%Al 2 O 3的陶瓷组合物的远IR辐射材料的粉末以30重量%或更多的量 和金属粉末,金属化合物或功能矿物粉末; 成型和干燥混合物; 和射击。
-
-