1.
公开(公告)号:US11994286B2
公开(公告)日:2024-05-28
申请号:US17500360
申请日:2021-10-13
Applicant: Zhejiang University
Inventor: Zhongyang Luo , Chunjiang Yu , Qinhui Wang , Mengxiang Fang , Hengli Zhang , Leming Cheng
IPC: F23B90/02 , C23F15/00 , F22B37/02 , F23G5/48 , F23G7/00 , F23J7/00 , F26B3/04 , F28F19/02 , G01B21/08 , C23C26/00
CPC classification number: F23B90/02 , C23F15/00 , F23J7/00 , F26B3/04 , F28F19/02 , G01B21/08 , F28F2245/00
Abstract: A method of preventing high temperature corrosion on a heat exchanging surface of a biomass boiler, including: a first feeding step, supplying a first biomass fuel to the boiler; a deposition step, performing combustion on the first biomass fuel during initial operation of the boiler, and forming an inert deposition layer on a surface of a heat exchanger of the boiler; a second feeding step, supplying a second biomass fuel different from the first biomass fuel to the boiler; and a normal combustion step, performing combustion on the second biomass fuel. A direct contact of an alkali metal chloride with a metal pipe wall is prevented by forming an inert deposition layer on the surface of the heat exchanger of the boiler in the deposition step, thereby establishing a physical barrier between the heat exchanging surface and the alkali metal chloride to prevent corrosion on the metal pipe wall.
-
2.
公开(公告)号:US20220113022A1
公开(公告)日:2022-04-14
申请号:US17500360
申请日:2021-10-13
Applicant: Zhejiang University
Inventor: Zhongyang Luo , Chunjiang Yu , Qinhui Wang , Mengxiang Fang , Hengli Zhang , Leming Cheng
Abstract: The present invention provides a method of preventing high temperature corrosion on a heat exchanging surface of a biomass boiler, including: a first feeding step, supplying a first biomass fuel to the boiler; a deposition step, performing combustion on the first biomass fuel during initial operation of the boiler, and forming an inert deposition layer on a surface of a heat exchanger of the boiler; a second feeding step, supplying a second biomass fuel different from the first biomass fuel to the boiler; and a normal combustion step, performing combustion on the second biomass fuel. A direct contact of an alkali metal chloride with a metal pipe wall is prevented by forming an inert deposition layer on the surface of the heat exchanger of the boiler in the deposition step, thereby establishing a physical barrier between the heat exchanging surface of the boiler and the alkali metal chloride to effectively solve a problem of preventing corrosion on the metal pipe wall of the boiler.
-