Composition or concentrate for conserving wood and wood materials
    1.
    发明授权
    Composition or concentrate for conserving wood and wood materials 失效
    用于保存木材和木材的成分或浓缩物

    公开(公告)号:US4750934A

    公开(公告)日:1988-06-14

    申请号:US901719

    申请日:1986-08-29

    摘要: A composition or concentrate for preserving wood, which comprises 0.001-5% by weight of cyano-(4-fluoro-3-phenoxyphenyl)-methyl 3-(2,2-dichloroethenyl)-2,2-dimethylcyclopropanecarboxylate and/or (pentafluorophenyl)-methyl 1R, 3R-3-(2,2-dichloroethenyl)-2,2-dimethylcyclopropanecarboxylate or enantiomeric compounds thereof and more than 75% by weight, preferably more than 90% by weight, of a mixture comprising at least one binder at least one diluent, and optionally at least one emulsifier and/or wetting agent or mixture thereof. The binder in the wood preservative or concentrate (calculated as solids) amounts to at least 1% by weight, preferably at least 4% by weight of the composition. An alkyd resin and/or a vegetable drying oil is preferably used in the composition as the organic binder for preventing or reducing damage to beneficial insects.

    摘要翻译: 用于保存木材的组合物或浓缩物,其包含0.001-5重量%的氰基 - (4-氟-3-苯氧基苯基) - 3-(2,2-二氯乙烯基)-2,2-二甲基环丙烷甲酸甲酯和/或(五氟苯基 ) - 1R,3R-3-(2,2-二氯乙烯基)-2,2-二甲基环丙烷甲酸甲酯或其对映异构体化合物和大于75重量%,优选大于90重量%的包含至少一种粘合剂 至少一种稀释剂和任选的至少一种乳化剂和/或润湿剂或其混合物。 木材防腐剂或浓缩物中的粘合剂(按固体计算)为组合物重量的至少1重量%,优选至少4重量%。 组合物中优选使用醇酸树脂和/或植物性干性油作为有机粘合剂,以防止或减少对有害昆虫的损害。

    Preservative composition for wood and wood building materials and method
of using same
    2.
    发明授权
    Preservative composition for wood and wood building materials and method of using same 失效
    木材和木材建筑材料的防腐剂组合物及其使用方法

    公开(公告)号:US4041176A

    公开(公告)日:1977-08-09

    申请号:US602903

    申请日:1975-08-07

    IPC分类号: B27K3/34 B27K3/50 A01N9/24

    摘要: Disclosed is a preservative composition for wood and wood construction material, comprising an organic solvent base, preferably an oily or oil-like solvent, at least one insecticide, organic fungicide or wood-preserving organic chemical compound which is soluble in the solvent, and typically from about 0.005 to 0.1% by weight, and more preferably between about 0.01 and 0.03% by weight, of at least one organic lithium compound soluble in the solvent, preferably lithium naphthenate or lithium octoate. The lithium compound provides also a marking effect for the compositions during application and subsequent thereto.

    摘要翻译: 公开了一种用于木材和木材建筑材料的防腐剂组合物,其包含有机溶剂基质,优选油状或油状溶剂,至少一种可溶于溶剂的杀虫剂,有机杀真菌剂或木材保存的有机化合物,通常 约0.005至0.1重量%,更优选约0.01至0.03重量%的至少一种可溶于溶剂的有机锂化合物,优选环烷酸锂或辛酸锂。 锂化合物在施用期间和之后也为组合物提供标记效果。