摘要:
An inorganic perchlorate is sensitized by adding about 1-8 percent by wei of copper chromite to said perchlorate. The mixture of inorganic perchlorate-copper chromite can be used as a substitute for RDX.
摘要:
A plastic-bonded pyrotechnical mixture is provided that includes at least one oxidatizer, one carbonate and/or phosphate from the group of alkali metals or earth alkali metals, a chlorinated rubber and a softener. An additional bonding agent and/or graphite can be added thereto as needed. The oxidatizer can be a perchlorate or a mixture of perchlorates from the group of alkali metals or earth alkali metals, or alternatively, ammonium perchlorates can also be integrated as an oxidatizer. The softener is an organic substance or substance mixture from the group of adipates or phthalates, or can be an organic phosphoric acid ester or a phosphoric acid ester mixture. As an additional bonding agent, an organic titanate or an organic titanate mixture is preferred. All components are mixed with one another at such a ratio that a neutral smoke in the pH range of 5-7 (bases on aerosol) is created.
摘要:
A pyrotechnic composition comprising:About 1 to 20% by weight of a thermoplastic resin selected from the group consisting of polyacetal resins, polyvinyl acetate resins and mixtures thereof;About 30 to 80% by weight of an alkali metal chlorite, such as sodium chlorite or potassium chlorite; andAbout 20 to 60% by weight of a coolant selected from the group consisting of calcium hydroxide, magnesium hydroxide or mixtures thereof.The invention also relates to a method of inflating an inflatable automobile safety restraint comprising the step of substantially completely inflating the restraint with the gaseous composition products of combustion of a composition comprising:About 1 to 20% by weight of a thermoplastic resin selected from the group consisting of polyacetal resins, polyvinyl acetate resins and mixtures thereof;About 30 to 80% by weight of an alkali metal chlorite, such as sodium chlorite or potassium chlorite; andAbout 20 to 60% by weight of a coolant selected from the group consisting of calcium hydroxide, magnesium hydroxide or mixtures thereof.