Ophthalmic and optical glasses
    1.
    发明授权
    Ophthalmic and optical glasses 有权
    眼科眼镜

    公开(公告)号:US06187702B1

    公开(公告)日:2001-02-13

    申请号:US09409012

    申请日:1999-09-29

    申请人: Michiko Morishita

    发明人: Michiko Morishita

    IPC分类号: C03C3066

    CPC分类号: C03C3/068 Y10S501/901

    摘要: Ophthalmic and optical glasses have a composition in weight percent of 4.5-9.5% SiO2, 10-19.5% B2O3, 0-3% Al2O3, 0-5% GeO2, 18—less than 23% La2O3, 0.3—less than 2% Gd2O3, 5.5-13.5% TiO2, 0-7.5% ZrO2, 15-21% Nb2O5, 0-1.5% Ta2O5, 0.3-5% WO3, with the proviso that (Ta2O5+WO3)/B2O3 is 0.5 or below in the ration terms of weight, 2.1-10% ZnO, 0-5% MgO, 7-12.5% CaO, 0-5% SrO, 0-4% BaO, ≧0.1% Li2O+Na2O+K2O in which 0-1% Li2O, 0-1% Na2O and 0-1% K2O, 0-0.5% As2O3 and 0-0.5% Sb2O3 and have a specific gravity of 4.1 or below, and optical constants of a refractive index (nd) exceeding 1.88 and up to 1.93 and an Abbe number j(&ngr; d) within a range from 28 to 31. A preferable range of Nb2O5 is 15.5—less than 20.5% and a more preferable range of Nb2O5 is less 15.5-20%.

    摘要翻译: 眼科和眼镜具有重量百分比为4.5-9.5%SiO 2,10-19.5%B 2 O 3,0-3%Al 2 O 3,0-5%GeO 2,18-小于23%La 2 O 3,0.3%小于2%Gd 2 O 3 ,5.5-13.5%TiO2,0-7.5%ZrO2,15-21%Nb2O5,0-1.5%Ta2O5,0.3-5%WO3,条件是(Ta2O5 + WO3)/ B2O3的比例为0.5以下 的重量,2.1-10%ZnO,0-5%MgO,7-12.5%CaO,0-5%SrO,0-4%BaO,≥0.1%Li2O + Na2O + K2O,其中0-1%Li2O, 0-1%Na2O和0-1%K2O,0-0.5%As2O3和0-0.5%Sb2O3,比重4.1或更低,折射率(nd)的光学常数超过1.88和高达1.93, 阿贝数j(&ngr; d)在28〜31的范围内.Nb 2 O 5的优选范围为20.5%以下15.5以下,Nb 2 O 5的更优选范围为15.5〜20%。

    Composition for barrier ribs of plasma display panel and method of fabricating such barrier ribs using the composition
    2.
    发明授权
    Composition for barrier ribs of plasma display panel and method of fabricating such barrier ribs using the composition 失效
    等离子体显示面板的隔壁的组合物和使用该组合物制造这种阻挡肋的方法

    公开(公告)号:US06271161B1

    公开(公告)日:2001-08-07

    申请号:US09385438

    申请日:1999-08-30

    IPC分类号: C03C3066

    CPC分类号: C03C3/074

    摘要: A composition for barrier ribs of plasma display panels and to a method of fabricating such barrier ribs using the composition is disclosed. The composition for the barrier ribs is SiO2—ZnO—PbO—B2O3 based glass. The SiO2—ZnO—PbO—B2O3 based glass consists of 10˜20 wt % of SiO2, 10˜30 wt % of ZnO, 5˜30 wt % of PbO, 10˜30 wt % of B2O3, 2˜10 wt % of K2O, 0˜5 wt % of Li2O, 1˜5 wt % of CaO, 3˜8 wt % of Na2O, 1˜5 wt % of Al2O3, and 0˜2 wt % of Sb2O3. In the method of forming the barrier ribs, the SiO2—ZnO—PbO—B2O3 based glass powder free from an oxide filler is primarily prepared. Paste or slurry is formed by mixing the SiO2—ZnO—PbO—B2O3 based glass with an organic vehicle. A thick film, having a predetermined thickness, is formed on the top surface of a lower substrate using the paste or slurry. Desired barrier ribs are, thereafter, formed by processing the paste or slurry film. In the barrier rib formation step, a pattern is formed on the top surface of the paste or slurry film before the paste or slurry film is etched or abraded using the pattern as a mask. The barrier ribs may be formed by stamping the paste or slurry film using a mold having a shape opposed to the desired pattern of the barrier ribs. The barrier ribs may be also formed by patterning a photoresist paste or slurry film.

    摘要翻译: 公开了一种用于等离子体显示面板的隔壁的组合物以及使用该组合物制造这种阻挡肋的方法。 隔壁用组合物为SiO2-ZnO-PbO-B2O3系玻璃。 SiO 2-ZnO-PbO-B 2 O 3基玻璃由10-20重量%的SiO 2,10〜30重量%的ZnO,5〜30重量%的PbO,10〜30重量%的B 2 O 3,2〜10重量% K 2 O,0〜5重量%的Li 2 O,1〜5重量%的CaO,3〜8重量%的Na 2 O,1〜5重量%的Al 2 O 3和0〜2重量%的Sb 2 O 3。 在形成隔壁的方法中,主要制备不含氧化物填料的SiO 2 -ZnO-PbO-B 2 O 3基玻璃粉末。 通过将SiO 2 -ZnO-PbO-B 2 O 3基玻璃与有机载体混合来形成浆料或浆料。 使用糊料或浆料,在下基板的顶表面上形成具有预定厚度的厚膜。 之后,通过加工糊状物或淤浆膜形成所需的隔壁。 在障壁形成步骤中,使用图案作为掩模,在糊料或浆料膜被蚀刻或研磨之前,在糊料或浆料膜的顶表面上形成图案。 阻挡肋可以通过使用具有与所需屏障的所需图案相对的形状的模具冲压该糊状物或浆料膜来形成。 阻挡肋也可以通过图案化光致抗蚀剂浆料或浆料膜而形成。

    Lead-free optical glasses
    3.
    发明授权
    Lead-free optical glasses 有权
    无铅光学眼镜

    公开(公告)号:US06333288B1

    公开(公告)日:2001-12-25

    申请号:US09567088

    申请日:2000-05-08

    IPC分类号: C03C3066

    摘要: The invention can relate to essentially lead-free optical glasses having a refractive index nd of from about 1.65 to about 1.87 and an Abbe number &ngr;d of from about 27 to about 43 and a composition (in % by weight, based on oxide) of SiO2 about 10-about 25, B2O3>about 10-about 25, Na2O about 2.5-about 10, K2O 0-about 3, CaO about 0.5-about 5, BaO about 15-about 30, ZnO about 5-about 15, TiO2 about 6-about 15, ZrO2 about 0.5-about 8, Y2O3 about 0.1-about 2, La2O3 about 0.5-about 8, Nb2O5 about 6-about 12, with La2O3+Nb2O5≦about 17,Ta2O5 0-about 1, and Gd2O3 0-about 1.

    摘要翻译: 本发明可以涉及折射率nd为约1.65至约1.87,阿贝数n为约27至约43的基本上无铅的光学玻璃以及组合物(以重量%计,基于氧化物) 的SiO 2约10至约25,B 2 O 3>约10至约25,Na 2 O约2.5至约10,K 2 O 0约3,CaO约0.5至约5,BaO约15至约30,ZnO约5至约15, TiO 2约6-约15,ZrO 2约0.5-约8,Y 2 O 3约0.1-约2,La 2 O 3约0.5-约8,Nb 2 O 5约6-约12,La 2 O 3 + Nb 2 O 5≤约17,Ta 2 O 5 0约1, 和Gd 2 O 3 0约1。

    High refractive index glasses, multifocal corrective lenses containing same
    4.
    发明授权
    High refractive index glasses, multifocal corrective lenses containing same 失效
    高折射率眼镜,含有其的多焦点矫正镜片

    公开(公告)号:US06284687B1

    公开(公告)日:2001-09-04

    申请号:US09529306

    申请日:2000-04-07

    IPC分类号: C03C3066

    摘要: The present invention relates to glasses of high refractive index having the following composition of oxides, expressed in percentages by weight: SiO2 29-35, B2O3 0.5-5, Li2O 0.5-3, Na2O 4-8, K2O 0-2, PbO 28-40, BaO 4-14, La2O3 4-12, TiO2 3-8, ZnO 0-8, ZrO2 0-4, Nb2O5 0-5, with: Li2O+Na2O+K2O 5.5-9; their use for the production of segments for multifocal corrective lenses; and multifocal corrective lenses incorporating at least one such segment in their structure.

    摘要翻译: 本发明涉及高折射率的玻璃,其具有如下组成的氧化物,以重量百分比表示:SiO 2 29-35,B 2 O 3 0.5-5,Li 2 O 0.5-3,Na 2 O 4 -8,K 2 O 2,PbO 28 -40,BaO 4-14,La 2 O 3 4-12,TiO 2 3-8,ZnO 0-8,ZrO 2 0-4,Nb 2 O 5 0-5,其中:Li 2 O + Na 2 O + K 2 O 5.5-9; 它们用于生产多焦点矫正镜片的片段; 以及在其结构中并入至少一个这样的片段的多焦点矫正镜片。

    Optical glass and its use
    6.
    发明授权
    Optical glass and its use 有权
    光学玻璃及其用途

    公开(公告)号:US06251813B1

    公开(公告)日:2001-06-26

    申请号:US09299619

    申请日:1999-04-27

    申请人: Kouichi Sato

    发明人: Kouichi Sato

    IPC分类号: C03C3066

    摘要: An optical glass having properties of a high refractive index and low dispersion and having both a low sag temperature Ts and a low liquidus temperature L.T., is provided. The optical glass comprises, by % by weight, 25 to 42% of B2O3, 14 to 30% of La2O3, 2 to 13% of Y2O3, 2 to 20 of SiO2, greater than 2% and 9% or less of Li2O, 0.5 to 20% of CaO, 2 to 20% of ZnO, 0 to 8% of Gd2O3, 0 to 8% of ZrO2, Gd2O3+ZrO2 being 0.5 to 12%, the total content thereof being at least 90%, and optionally contains 0 to 5% of Na2O, 0 to 5% of K2O, 0 to 5% of MgO, 0 to 5% of SrO, 0 to 10% of SrO, 0 to 10% of BaO, 0 to 5% of Ta2O, 0 to 5% of Al2O3, 0 to 5% of Yb2O3, 0 to 5% of Nb2O5, 0 to 2% of As2O3 and 0 to 2% of Sb2O3.

    摘要翻译: 提供了具有高折射率和低色散特性并具有低下垂温度Ts和低液相线温度L.T.的光学玻璃。 光学玻璃的重量比为25重量%以上的B 2 O 3,14〜30重量%的La 2 O 3,2〜13重量%的Y 2 O 3,2〜20重量%的SiO 2,2重量%以上9重量%以下的Li 2 O,0.5重量% 至20%的CaO,2〜20%的ZnO,0〜8%的Gd2O3,0〜8%的ZrO2,Gd2O3 + ZrO2为0.5〜12%,总含量为90%以上, 至5%的Na 2 O,0至5%的K 2 O,0至5%的MgO,0至5%的SrO,0至10%的SrO,0至10%的BaO,0至5%的Ta 2 O,0至 5%的Al 2 O 3,0〜5%的Yb 2 O 3,0〜5%的Nb 2 O 5,0〜2%的As 2 O 3和0〜2的Sb 2 O 3。

    Composition containing lead-oxide free glass powder of low softening point useful for barrier rib in PDP
    7.
    发明授权
    Composition containing lead-oxide free glass powder of low softening point useful for barrier rib in PDP 失效
    含有无铅玻璃粉末的组合物,其低软化点用于PDP中的隔壁

    公开(公告)号:US06589894B1

    公开(公告)日:2003-07-08

    申请号:US09659750

    申请日:2000-09-11

    IPC分类号: C03C3066

    摘要: In a composition for use in formation of barrier ribs in a plasma display panel, comprising glass powder, the glass powder is powder of PbO free and alkali metal oxide free glass which consists essentially of, by molecular percent, 5-40% BaO, 20-55% ZnO, 15-50% B2O3, 0-25% SiO2. The glass has a softening point of 630° C. or less. Ceramics powder is mixed with the glass powder. The composition can also be provided in a form of paste, alternatively in a form of a green sheet.

    摘要翻译: 在用于形成等离子体显示面板中的阻挡层的组合物中,包含玻璃粉末,该玻璃粉末是不含PbO和不含碱金属氧化物的玻璃的粉末,其基本上由分子百分比含量为5-40%的BaO,20 -55%ZnO,15-50%B2O3,0-25%SiO2。 该玻璃的软化点为630℃以下。 陶瓷粉末与玻璃粉末混合。 组合物也可以以糊状物的形式提供,或者以生片的形式提供。

    Dielectric composition for plasma display panel
    8.
    发明授权
    Dielectric composition for plasma display panel 有权
    等离子体显示面板的介电组成

    公开(公告)号:US06184163B2

    公开(公告)日:2001-02-06

    申请号:US09209240

    申请日:1998-12-10

    IPC分类号: C03C3066

    摘要: A dielectric composition for a plasma display panel. In the dielectric composition, a SiO3—ZnO—B2O3 group glass is used. Accordingly, the dielectric composition is capable of meeting optical, thermal and electrical characteristic requirements of a dielectric layer and allows the dielectric layer to have a light weight.

    摘要翻译: 一种用于等离子体显示面板的电介质组合物。 在电介质组合物中,使用SiO 3 -ZZ-B 2 O 3族玻璃。 因此,电介质组合物能够满足介电层的光学,热学和电学特性要求,并且允许电介质层具有轻质量。