摘要:
The invention relates to a photoactive component, especially a solar cell, consisting of organic layers and formed by at least one stacked pi, ni, and/or pin diode. Said diodes are characterised in that they comprise at least one p-doped or n-doped transport layer having a larger optical band gap than that of the photoactive layer. The individual diodes are characterised by a high internal quantum yield, but can be optically thin (peak absorption
摘要:
The invention relates to polynucleotides targeted against a gene of a catalytic sub-unit of human telomerase and the use of said polynucleotides for the diagnosis, prophylaxis, reduction and course control of diseases linked to cell growth, differentiation and/or division, such as, for example, tumorous diseases.
摘要:
The invention relates to a method for automatically correcting mechanical deformations of optical correlators and to a self-correcting optical correlator for use in the optical correlation analysis of two digital images, which allows the displacement of the images in relation to one another on the image plane to be determined in realtime. The invention uses the method for automatically correcting the errors of optical correlators, which are caused by deformations of the system and occur during the determination of the plane displacement of two digital images in relation to one another. The method is characterised by a vertical or horizontal reflection of the spectral image, the determination of the plane displacement of the images to be analysed in relation to one another at half the distance between the correlation points, the use of only one part of the pixels of the spectral image for the second transformation step and the superimposition of the images to be analysed with a calibration pattern. A JTC optical correlator is used to implement said method.
摘要:
The invention relates to a bearing steel with a usual bearing steel composition i.e. 100Cr6 or 100CrMn6, exhibiting delayed austenite recrystallization. Said steel contains: 0.80-1.05 mass % carbon; 0.17-0.65 mass % silicon; 0.20-1.20 mass % manganese; 1.30-1.65 mass % chrome; a maximum of 0.027 mass % phosphorous; a maximum of 0.30 mass % nickel; 0.020 mass % sulfur; 0.25 mass % copper; 0.3-1.0 mass % vanadine and/or 0.01-0.1 mass % niobium. Also disclosed is the use of said bearing steel in thermomechanical forming.