Abstract: A method for producing high porosity boehmite alumina wherein an aqueous boehmite slurry is mixed with an effective amount of a modifier comprising a hydroxide or oxide of an element of group IIIA-VIA on the Periodic Table of Elements and having a pKsp of greater than 11 to produce a precursor mixture and hydrothermally aging the precursor mixture at an elevated temperature under agitation with an effective consumptive power of greater than 1 kW/m 3 .
Abstract translation: 一种生产高孔隙率勃姆石氧化铝的方法,其中勃姆石水泥浆与有效量的包含IIIA-VIA族元素的氢氧化物或氧化物的改性剂混合在元素周期表上,并且具有大于11的pKsp 产生前体混合物并在升高的温度下在高于1kW / m 3的有效消耗功率的搅拌下水解老化前体混合物。