WOOD FLOORING WITH CARBONIZED SOLID WOOD USING SYMMETRIC STRUCTURE AND PROCESS FOR PREPARING THE SAME
    3.
    发明申请
    WOOD FLOORING WITH CARBONIZED SOLID WOOD USING SYMMETRIC STRUCTURE AND PROCESS FOR PREPARING THE SAME 审中-公开
    使用对称结构的碳化固体木材的木地板及其制备方法

    公开(公告)号:WO2008038869A1

    公开(公告)日:2008-04-03

    申请号:PCT/KR2007/001024

    申请日:2007-02-28

    CPC classification number: E04F15/02 B32B21/14 E04F15/04

    Abstract: Provided is wood flooring having a symmetric structure comprising application of carbonized solid wood to top and bottom layers and a process for preparing the same. The wood flooring of the present invention has a symmetric structure by symmetric lamination of high-temperature heat-treated veneers having a thickness of more than 2 mm on top and bottom layers and integration of the layers under given temperature and pressure conditions. Therefore, the wood flooring is capable of maintaining the balance, is capable of completely solving a problem of deformation due to environmental fluctuations, is capable of achieving dimensional stability and high-quality color of product, and is capable of removing surface contamination, thus making it possible to use contaminated lower-grade coniferous lumber as a wood flooring material.

    Abstract translation: 提供了具有对称结构的木地板,其包括将碳化的实木施加到顶层和底层,以及其制备方法。 本发明的木地板通过在顶层和底层上具有大于2mm厚度的高温热处理单板的对称层压和在给定的温度和压力条件下层的一体化而具有对称结构。 因此,木地板能够保持平衡,能够完全解决由于环境波动引起的变形的问题,能够实现产品的尺寸稳定性和高品质的颜色,并且能够去除表面污染,从而使 可以使用受污染的低级针叶木作为木地板材料。