Abstract: According to one embodiment, a method for forming a laminated glass sheet includes forming a multi-layer glass melt (300) from a molten core glass (106) and at least one molten cladding glass (126). The multi-layer glass melt (300) has a width W m , a melt thickness Tm and a core to cladding thickness ratio T c :T d . The multi-layer glass melt (300) is directed onto the surface of a molten metal bath (162) contained in a float tank (160). The width W m of the multi-layer glass melt (300) is less than the width W f of the float tank (160) prior to the multi-layer glass melt (300) entering the float tank (160). The multi-layer glass melt (300) flows over the surface of the molten metal bath (162) such that the width W m of the multi-layer glass melt (300) increases, the melt thickness Tm decreases, and the core to cladding thickness ratio T c :TC i remains constant as the multi-layer glass melt (300) solidifies into a laminated glass sheet.
Abstract translation: 根据一个实施例,一种用于形成夹层玻璃板的方法包括从熔融芯玻璃(106)和至少一个熔融包层玻璃(126)形成多层玻璃熔体(300)。 多层玻璃熔体(300)具有宽度Wm,熔体厚度Tm和芯与包层厚度比Tc:Td。 多层玻璃熔体(300)被引导到包含在浮子罐(160)中的熔融金属浴(162)的表面上。 多层玻璃熔体(300)的宽度Wm小于多层玻璃熔体(300)进入浮子槽(160)之前的浮子槽(160)的宽度Wf。 多层玻璃熔体(300)在熔融金属浴(162)的表面上流动,使得多层玻璃熔体(300)的宽度Wm增加,熔体厚度Tm降低,芯到包层厚度 比例Tc:当多层玻璃熔体(300)凝固成夹层玻璃板时,TCi保持恒定。